Effect of annealing on the microstructure of NiFe1.925Dy0.075O4 thin films
Source abstract
Abstract
Abstract Dysprosium-doped nickel-ferrite (NiFe 1.925 Dy 0.075 O 4 ) thin films were fabricated using RF sputter-deposition. Structural studies indicate that the effect of post-deposition annealing is significant on structural evolution in NiFe 1.925 Dy 0.075 O 4 films. As-grown NiFe 1.925 Dy 0.075 O 4 films were amorphous. Annealing (T a ) in air at 450–1000 °C results in the formation of nanocrystalline NiFe 1.925 Dy 0.075 O 4 films, which crystallize in the inverse spinel structure. The average grain size ( L ) increases from 5 to 40 nm with increasing T a from 450 to 1000 °C. Lattice constant of NiFe 1.925 Dy 0.075 O 4 films is higher compared to that of NiFe 2 O 4 due to partial substitution of Dy 3+ ions for Fe 3+ ions. The lattice parameter increases from 8.353 to 8.362 A with increasing T a from 450 to 1000 °C which is attributed to the lattice-strain developed in the NiFe 1.925 Dy 0.075 O 4 films with increasing T a . The corresponding density of NiFe 1.925 Dy 0.075 O 4 films increases from 3.2 to 3.9 g/cm 3 with increasing annealing temperature. Magnetization measurements indicate the ferromagnetic behavior of all the films while the coercive field values at 300 K are found to be 0.0134 T and 0.0162 T for as grown and T a = 1000 °C films, respectively.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Magnetic Properties and Synthesis of Ferrites · Magneto-Optical Properties and Applications · Multiferroics and related materials
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References
Reference metadata was not supplied for this record.