Chemical vapour deposition of praseodymium oxide films on silicon: influence of temperature and oxygen pressure
Source abstract
Abstract
Abstract Metal-organic chemical vapour deposition (MOCVD) of various phases in PrO x system has been studied in relation with deposition temperature (450–750 °C) and oxygen partial pressure (0.027–100 Pa or 0.2–750 mTorr). Depositions were carried out by pulsed liquid injection MOCVD using Pr(thd) 3 (thd = 2,2,6,6-tetramethyl-3,5-heptanedionate) precursor dissolved in toluene or monoglyme. By varying deposition temperature and oxygen partial pressure amorphous films or various crystalline PrO x phases (Pr 2 O 3 , Pr 7 O 12 , Pr 6 O 11 ) and their mixtures can be grown. The pure crystalline Pr 2 O 3 phase grows only in a narrow range of partial oxygen pressure and temperature, while high oxygen pressure (40–100 Pa) always leads to the most stable Pr 6 O 11 phase. The influence of annealing under vacuum at 750 °C on film phase composition was also studied. Near 90% step coverage conformity was achieved for PrO x films on structured silicon substrates with aspect ratio 1:10. In air degradation of Pr 2 O 3 films with transformation to Pr(OH) 3 was observed in contrast to Pr 6 O 11 films.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Semiconductor materials and devices · Electronic and Structural Properties of Oxides · Catalytic Processes in Materials Science
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References
Reference metadata was not supplied for this record.