Fully strained low-temperature epitaxy of TiN/MgO(001) layers using high-flux, low-energy ion irradiation during reactive magnetron sputter deposition

Taeyoon Lee, H. Seo, H. Hwang, B. Howe, S. Kodambaka, J.E. Greene, I. Petrov

Thin Solid Films· Volume 518· Issue 18
Publisher page

Abstract

Abstract Epitaxial TiN layers, 0.3 μm thick, are grown on MgO(001) in the absence of applied substrate heating using very high flux, low-energy (below the lattice atom displacement threshold), ion irradiation during reactive magnetron sputter deposition in pure N 2 discharges. High-resolution x-ray diffraction, reciprocal lattice maps, and transmission electron microscopy analyses reveal that the TiN(001) films grow with an (001) TiN ||(001) MgO and [100] TiN ||[100] MgO orientation relationship to the substrate. The layers are fully coherent with no detectable misfit dislocations. For comparison, TiN/MgO(001) films grown at temperatures of 700–850 °C under similar conditions, but with no intentional ion irradiation, are fully relaxed with a high misfit dislocation density. Thus, the present results reveal that intense low-energy ion irradiation during film growth facilitates high adatom mobilities giving rise to low-temperature epitaxy, while the low growth temperature quenches strain-induced relaxation and suppresses misfit dislocation formation.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Metal and Thin Film Mechanics · GaN-based semiconductor devices and materials · ZnO doping and properties

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (29)

Show source-provided references
1. Cereda · Phys. Rev. Lett. · 2008 · 100 · 04610510.1103/PhysRevLett.100.046105 ↗
2. Kitagawa · Appl. Surf. Sci. · 2000 · 159 · 3010.1016/S0169-4332(00)00081-7 ↗
3. Ruthe · J. Vac. Sci. Technol. A · 2004 · 22 · 244610.1116/1.1807394 ↗
4. Lee · Appl. Phys. Lett. · 1994 · 65 · 323610.1063/1.112423 ↗
5. Park · J. Crystal Growth · 2007 · 309 · 15810.1016/j.jcrysgro.2007.09.020 ↗
6. Kimura · J. Crystal Growth · 2008 · 310 · 4010.1016/j.jcrysgro.2007.09.038 ↗
7. Petrov · J. Vac. Sci. Technol. A · 1992 · 10 · 26510.1116/1.578074 ↗
8. Adibi · J. Appl. Phys. · 1993 · 73 · 858010.1063/1.353388 ↗
9. Karr · Phys. Rev. B · 2000 · 61 · 1613710.1103/PhysRevB.61.16137 ↗
10. Shin · J. Appl. Phys. · 2003 · 93 · 602510.1063/1.1568521 ↗
11. Lee · Phys. Rev. B · 2005 · 71 · 14410610.1103/PhysRevB.71.144106 ↗
12. Hultman · Thin Solid Films · 1991 · 205 · 15310.1016/0040-6090(91)90297-B ↗
13. Hultman · J. Appl. Phys. · 1987 · 61 · 55210.1063/1.338257 ↗
14. Hultman · J. Cryst. Growth · 1998 · 92 · 63910.1016/0022-0248(88)90048-6 ↗
15. Shin · J. Appl. Phys. · 2004 · 95 · 35610.1063/1.1629155 ↗
16. Petrov · J. Vac. Sci. Technol. A · 1992 · 10 · 328310.1116/1.577812 ↗
17. Greene · Appl. Phys. Lett. · 1995 · 67 · 292810.1063/1.114845 ↗
18. Phelps · J. Phys. Chem. Ref. Data · 1991 · 20 · 55710.1063/1.555889 ↗
19. Chapman · 1980 · 108
20. Petrov · J. Vac. Sci. Technol. A · 1994 · 12 · 284610.1116/1.578955 ↗
21. Doolittle · Nucl. Instrum. Methods Phys. Res. B · 1985 · 15 · 34410.1016/0168-583X(85)90762-1 ↗
22. Noel · J. Appl. Phys. · 1989 · 65 · 118910.1063/1.343062 ↗
23. Inorganic Index to Powder Diffraction File (Joint Committee on Powder Diffraction Standards, Swarthmore, PA, 1997): Card No. 45-0946.Swarthmore, PA, 1997): Card No. 45-0946.
24. Inorganic Index to Powder Diffraction File (Joint Committee on Powder Diffraction Standards, Swarthmore, PA, 1997): Card No. 45-0946.Swarthmore, PA, 1997): Card No. 38-1420.
25. Powell · J. Appl. Phys. · 1998 · 73 · 18910.1063/1.353882 ↗
26. van der Sluis · J. Phys. D · 1993 · 26 A · 18810.1088/0022-3727/26/4A/039 ↗
27. Aigner · J. Alloys Compd. · 1994 · 215 · 12110.1016/0925-8388(94)90828-1 ↗
28. Landolt · 1975 · vol. 7, Pt. b1 · 27
29. Pierson · 1996