Abstract
Abstract SnS2 films have been deposited on glass and alumina plate substrates by the reactions between an organotin precursor [tetrabuyltin, (CH2CH2CH2CH3)4Sn] and carbon disulfide in n-hexane at the temperature range 180–200 °C for 10–40 h. The reaction system was oxygen free and applied at a moderate temperature. The films so prepared were characterized by techniques of X-ray diffraction, Scanning electron microscopy, Raman and Mossbauer spectroscopies. The films deposited on glass as well as on alumina plate have an average thickness of 30 μm, but have different rose-like morphologies, which are influenced by both the anisotropic growths of crystals and the different substrate structures. Photoluminescence measurements show that the films have an emission peak at approximately 590 nm.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Chalcogenide Semiconductor Thin Films · Organometallic Compounds Synthesis and Characterization · Corrosion Behavior and Inhibition
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References
Reference metadata was not supplied for this record.