article·2006-09-21

Filtered vacuum arc deposition of transparent conducting Al-doped ZnO films

V.N. Zhitomirsky, E. Çetinörgü, E.L. Adler, Yu. Rosenberg, R.L. Boxman, S. Goldsmith

Publisher page

Abstract

Abstract Transparent conducting ZnO:Al and ZnO films of 380–800 nm thickness were deposited on glass substrates by filtered vacuum arc deposition (FVAD), using a cylindrical Zn cathode doped with 5–6 at.% Al or a pure Zn cathode in oxygen background gas with pressure P = 0.4–0.93 Pa. The crystalline structure, composition and electrical and optical properties of the films were studied as functions of P . The films were stored under ambient air conditions and the variation of their resistance as function of storage time was monitored over a period of several months. The Al concentration in the film was found to be 0.006–0.008 at.%, i.e., a few orders of magnitude lower than that in the cathode material. However, this low Al content influenced the film resistivity, ρ , and its stability. The resistivity of as-deposited ZnO:Al films, ρ = (6–8) × 10 − 3 Ω cm, was independent of P and lower by a factor of 2 in comparison to that of the ZnO films deposited by the same FVAD system. The ρ of ZnO films 60 days after deposition increased by a factor of ∼ 7 with respect to as-deposited films. The ZnO:Al films deposited with P = 0.47–0.6 Pa were more stable, their ρ first slowly increased during the storage time (1.1–1.4 times with respect to as-deposited films), and then stabilized after 30–45 days.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: ZnO doping and properties · Ga2O3 and related materials · Gas Sensing Nanomaterials and Sensors

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References