article·2004-07-22

Peeling and delamination in Cu/SiLK™ process during Cu-CMP

S. Balakumar, Xian Chen, Y.W. Chen, T. Selvaraj, Benfu Lin, Rakesh Kumar, T. Hara, Masayo Fujimoto, Y. Shimura

Publisher page

Abstract

Abstract One of the major challenges with integration of Cu/low-k or ultralow-k materials is to eliminate delamination during chemical mechanical planarization (CMP) process due to their porous nature and weak mechanical properties. Three different kinds of peeling at various metal levels—single layer peeling, multi-stack delamination and pattern design related—were generally observed in the CMP process of Cu/SiLK™. The single stack peeling is due to poor mechanical integrity of low-k materials with barriers. Based on the results of this study, multi-stack and pattern design related peelings were attributed to the degradation of adhesion caused by accumulation of stress. Critical pressure for CMP using Al2O3 and MnO2 slurries was also determined for single and dual stacks. Robust CMP process for Cu/SiLK™ integration developed with new process concept will be discussed and seven layers of Cu/SiLK™ metallization processed with dual damascene was successfully demonstrated.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Advanced Surface Polishing Techniques · Copper Interconnects and Reliability · Advanced machining processes and optimization

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References

Reference metadata was not supplied for this record.