Hot-pressed Ti-Al targets for synthesizing Ti1−xAlxN films by the arc ion plating method
Source abstract
Abstract
Abstract Ti and Al powders were mixed with identical atomic ratios and hot-pressed at 650, 800, 950, 1100 and 1250°C, respectively, for the use of targets in the arc ion plating (AIP) method. As the sintering temperatures increased, the target density monotonously increased and the porosity correspondingly decreased. Chemical analysis by X-ray diffraction indicated that pure Ti and Al phases decreased and intermetallics such as TiAl3 and Ti3Al phases were formed at 800–950°C. Over 950°C, the amount of the intermetallics decreased and finally TiAl phase was formed. Next, the Ti-Al targets were arc-discharged in nitrogen plasma and Ti1−xAlxN films were deposited on mirror-polished cemented carbide substrates. The targets with lower density, sintered at 650 and 800°C, did not easily trigger and keep stable arc-discharge during the deposition. As a result, synthesized Ti1−xAlxN films had a larger number and size of droplets which were not only circular but were also irregular shapes. Although microstructures of Ti–Al targets were quite different, all films mostly consisted of Ti0.5Al0.5N with the NaCl structure and similar hardness with approximately 3000 HV. Further, all Ti0.5Al0.5N films had the same columnar cross-sectional structures and the growth rate was approximately 17 μm/h.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Metal and Thin Film Mechanics · Advanced materials and composites · Diamond and Carbon-based Materials Research
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References
Reference metadata was not supplied for this record.