Sn deposition onto Cu and alloy layer growth by a contact immersion process
Source abstract
Abstract
Abstract Sn was deposited onto a Cu substrate by the contact immersion processes, where a Cu substrate was dipped into a Sn 2+ -citrate solution, and was directly or electrically contacted to metallic Sn dipped in the same solution. Sn was deposited at underpotential and the deposition kinetics followed a parabolic rate law. The deposited Sn did not exist as elemental Sn films but formed Cu–Sn intermetallic phases. The growth of the Cu–Sn intermetallic layer is continued by the underpotential deposition of Sn onto this layer, and its rate is determined by the solid-state diffusion of Sn and Cu atoms through the intermetallic phase films.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Electronic Packaging and Soldering Technologies · Copper Interconnects and Reliability · Aluminum Alloy Microstructure Properties
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References
Reference metadata was not supplied for this record.