article·2000-09-01

Formation process and material properties of reactive sputtered IrO2 thin films

Ray‐Hua Horng, Dong‐Sing Wuu, L. H. Wu, M.K Lee

Publisher page

Abstract

Abstract IrO 2 thin films were deposited by reactive sputtering in various O 2 /(O 2 +Ar) mixing ratios (OMR). The systematic study of the OMR effect on the properties of IrO 2 thin films has been reported. It was found that the formation of IrO 2 could be classified into two classes, depending on the O 2 flow ratio. At low OMR (10–30%), the Ir target and Si substrate were not oxidized and a high deposition rate and high crystallinity IrO 2 could be obtained. On the other hand, at high OMR (>30%), the target and Si substrate were oxidized. It resulted in a lower deposition rate of IrO 2 and yielded poor structural properties. Moreover, the high OMR provided O atoms, incorporated into the IrO 2 thin film. This point could be confirmed by X-ray photoelectron spectroscopy. The excess O defects would also make the resistivity of IrO 2 increase as the samples were prepared at high OMR. The effect of substrate temperature on the resistivity was also discussed. It was found that the resistivity of the IrO 2 films decreased with an increase of the substrate temperature and a minimum resistivity of 70 μΩcm was obtained as films deposited at 600°C using 10% OMR.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Semiconductor materials and devices · ZnO doping and properties · Copper Interconnects and Reliability

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References