Low temperature boron doping into crystalline silicon by boron-containing species generated in Cat-CVD apparatus
Source abstract
Abstract
Abstract We have discovered that phosphorus (P) atoms can be doped into crystalline silicon (c-Si) at temperatures below 350 °C or even at 80 °C by using species generated by catalytic cracking reaction of phosphine (PH 3 ) molecules with heated tungsten (W) catalyzer in Cat-CVD apparatus. As further investigation, here, we study the feasibility of low temperature doping of boron (B) atoms into c-Si by using decomposed species generated similarly from diborane (B 2 H 6 ) molecules. Dependency of properties of doped layers on catalyzer temperature (T cat ) and substrate temperature (T s ) is studied by both the Van der Pauw method based on the Hall-effect measurements and secondary ion mass spectroscopy (SIMS) for B doping in addition to P doping. It is found that, similarly to P doping, the surface of n-type c-Si is converted to p-type even at T s = 80 °C for T cat over 800 °C when c-Si is exposed to B 2 H 6 cracked species for a few minutes, and that the heat of substrate over 300 °C is likely to help for B doping contrary to P doping.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Advancements in Semiconductor Devices and Circuit Design · Silicon and Solar Cell Technologies · Semiconductor materials and interfaces
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (24)
Show source-provided references
1. Oxygen in silicon
2. Mizuno · Appl. Phys. Lett. · 1988 · 53 · 205910.1063/1.100318 ↗
3. Sasaki · Nucl. Inst. Methods Phys. Res. B · 2005 · 237 · 4110.1016/j.nimb.2005.04.109 ↗
4. Sasaki · 2006 · 524
5. Koo · IEEE Trans. Plasma Sci. · 2004 · 32 · 45610.1109/TPS.2004.828134 ↗
6. Yon · Jpn. J. Appl. Phys. · 2006 · 45 · 296110.1143/JJAP.45.2961 ↗
7. Sasaki · 2010 · 103
8. Sasaki · 2008 · 917
9. Clarke · Physica · 2008 · E40 · 156610.1016/j.physe.2007.09.180 ↗
10. O'Brien · Phys. Rev. B · 2001 · 64 · 16140110.1103/PhysRevB.64.161401 ↗
11. Ruess · Nano Lett. · 2004 · 4 · 196910.1021/nl048808v ↗
12. Gossmann · Phys. Rev. · 1993 · B47 · 1261810.1103/PhysRevB.47.12618 ↗
13. Zeindl · Appl. Phys. Lett. · 1987 · 50 · 116410.1063/1.97950 ↗
14. Denhoff · Appl. Phys. Lett. · 1989 · 54 · 133210.1063/1.100707 ↗
15. Mattey · Appl. Phys. Lett. · 1990 · 57 · 164810.1063/1.104076 ↗
16. Zeindl · Thin Solid Films · 1990 · 184 · 2110.1016/0040-6090(90)90393-R ↗
17. Schubert · 1996 · 69
18. Epitaxial microstructures
19. Hayakawa · Jpn. J. Appl. Phys. · 2012 · 51 · 06130110.1143/JJAP.51.061301 ↗
20. Hayakawa · Jpn. J. Appl. Phys. · 2011 · 50 · 12130110.1143/JJAP.50.121301 ↗
21. Koyama · Thin Solid Films · 2011 · 519 · 447310.1016/j.tsf.2011.01.294 ↗
22. Roca i Cabarrocas · J. Appl. Phys. · 1989 · 66 · 328610.1063/1.344122 ↗
23. Habuka · J. Cryst. Growth · 2000 · 209 · 80710.1016/S0022-0248(99)00732-0 ↗
24. Itoh · J. Mater. Sci. · 1987 · 22 · 281110.1007/BF01086475 ↗