article·2017-01-23

Electrochemical preparation of tungsten oxide hydrate films with controlled bandgap energy

K. Nishiyama, Junji Sasano, Seiji Yokoyama, Masanobu Izaki

Publisher page

Abstract

Abstract Tungsten oxide hydrate films of WO 3 ∙ H 2 O and WO 3 ∙(H 2 O) 0.33 were prepared on conductive glass substrates by anodic deposition in aqueous 0.01–0.5 mol/L WO 4 2 − solutions. Structural and optical characterizations were carried out by X-ray photoelectron spectroscopy, X-ray diffraction, SEM observation, optical absorption measurements, and photoelectrochemical measurements. The films composed of large WO 3 ∙ H 2 O grains with square shapes, which was obtained in the 0.01–0.09 mol/L WO 4 2 − solutions, possessed a bandgap energy of approximately 2.5 eV, and the granular-WO 3 ∙(H 2 O) 0.33 films, which was obtained in the 0.05–0.5 mol/L WO 4 2 − solutions, showed 3.3 eV in bandgap energy. The WO 3 ∙ H 2 O-WO 3 ∙(H 2 O) 0.33 mixtured films prepared in the 0.01–0.09 mol/L WO 4 2 − solutions showed a photoresponse for visible light at 380–600 nm, due to the presence of 2.5 eV-bandgap WO 3 ∙ H 2 O.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Transition Metal Oxide Nanomaterials · Gas Sensing Nanomaterials and Sensors · ZnO doping and properties

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.