Spherical indentation and scratch durability studies of transparent conducting layers on polymer substrates
Source abstract
Abstract
Abstract The effect of moderate normal and tangential spherical loading on the durability of brittle ceramic films sputtered on polymer substrates is investigated. Indium tin oxide films with various thicknesses are deposited by sputtering on polyethylene terephthalate substrates and their mechanical durability is assessed using a spherical nanoindenter and scratch tester with built-in optical microscopy capability. It is observed that crack initiation occurs at 40 mN normal applied load. As loading increases, formation of brittle ring cracking and of secondary radial cracks is evident. It is also shown that ring crack spacing is thickness dependent. During scratch testing two main coating failure modes are observed. The first is through thickness cracking and the second is buckling spallation of the coating. Both failure mechanisms exhibit thickness dependence.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Metal and Thin Film Mechanics · Advanced ceramic materials synthesis · Acoustic Wave Resonator Technologies
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (28)
Show source-provided references
1. Crawford · 2005 · 1
2. Paine · 2005 · 79
3. Nunes de Carvalho · Thin Solid Films · 2003 · 427 · 21510.1016/S0040-6090(02)01213-0 ↗
4. Kim · Appl. Phys. Lett. · 2001 · 79 · 28410.1063/1.1383568 ↗
5. Sierros · Thin Solid Films · 2010 · 518 · 262310.1016/j.tsf.2009.08.002 ↗
6. Suchea · Thin Solid Films · 2007 · 515 · 656210.1016/j.tsf.2006.11.151 ↗
7. Minami · Thin Solid Films · 2008 · 516 · 131410.1016/j.tsf.2007.03.082 ↗
8. Suo · China Part. · 2005 · 3 · 32110.1016/S1672-2515(07)60210-3 ↗
9. Cairns · Appl. Phys. Lett. · 2000 · 76 · 142510.1063/1.126052 ↗
10. Letterier · Thin Solid Films · 2004 · 460 · 15610.1016/j.tsf.2004.01.052 ↗
11. Chen · Eng. Fract. Mech. · 2002 · 69 · 59710.1016/S0013-7944(01)00104-7 ↗
12. Gorkhali · J. Soc. Inf. Display · 2004 · 12 · 4510.1889/1.1824238 ↗
13. Sierros · J. Soc. Inf. Display · 2009 · 17 · 94910.1889/JSID17.11.947 ↗
14. Sierros · Thin Solid Films · 2009 · 517 · 259010.1016/j.tsf.2008.10.031 ↗
15. Sierros · Wear · 2007 · 263 · 99210.1016/j.wear.2007.01.073 ↗
16. Sierros · Wear · 2009 · 267 · 62510.1016/j.wear.2008.12.042 ↗
17. Knapp · J. Appl. Phys. · 1999 · 85 · 146010.1063/1.369178 ↗
18. Chai · J. Mater. Res. · 2004 · 19 · 175210.1557/JMR.2004.0219 ↗
19. Andersson · Eng. Fract. Mech. · 1998 · 61 · 9310.1016/S0013-7944(98)00057-5 ↗
20. Zeng · Thin Solid Films · 2003 · 443 · 6010.1016/S0040-6090(03)00915-5 ↗
21. Chang · Surf. Coat. Tech. · 2008 · 202 · 541610.1016/j.surfcoat.2008.06.024 ↗
22. Zhitomirsky · Thin Solid Films · 2005 · 492 · 18710.1016/j.tsf.2005.06.061 ↗
23. Bull · Surf. Coat. Tech. · 1991 · 50 · 2510.1016/0257-8972(91)90188-3 ↗
24. K.L. Johnson, Contact mechanics, Cambridge University Press, Cambridge, pp. 90–95 1987 (Chapter 4).
25. Kourtesis · J. Mater. Sci. · 1997 · 32 · 449310.1023/A:1018608931236 ↗
26. Rao · Polymer · 2008 · 49 · 250710.1016/j.polymer.2008.03.046 ↗
27. Leterrier · J. Polym. Sci. Pol. Phys. · 1997 · 35 · 146310.1002/(SICI)1099-0488(19970715)35:9<1463::AID-POLB16>3.0.CO;2-4 ↗
28. Bull · Tribol. Int. · 1997 · 30 · 49110.1016/S0301-679X(97)00012-1 ↗