journal article·2006-11Open access

Characterization of magnetron co-sputtered W-doped C-based films

C.W. Moura e Silva, J.R.T. Branco, A. Cavaleiro

Thin Solid Films· Volume 515· Issue 3

Abstract

In this paper, W-doped C-based coatings were deposited on steel and silicon substrates by RF magnetron sputtering, using W and C targets, varying the cathode power applied to the W target and the substrate bias. The chemical composition was varied by placing the substrates in a row facing the C and W targets. W content in the films increased from 1 to 2 at.% over the C target to ∼73 at.% over the W target. The coatings with W content lower than ∼12 at.% and ∼23 at.%, for biased and unbiased conditions, respectively, showed X-ray amorphous structures, although carbide nanocrystals must exist as shown by the detection of the WC1−x phase in films with higher W content. C-rich films were very dense and developed a columnar morphology with increasing W content. An improvement in the hardness (from 10 GPa, up to 25 GPa) of the films was achieved either when negative substrate bias was used in the deposition, or when the WC1−x phase was detected by X-ray diffraction. The adhesion of the coatings is very low with spontaneous spallation of those deposited with negative substrate bias higher than 45 V. Varieties in cathode power (90 W or 120 W) applied to the W target showed no observable influence on the characteristics of the films.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Diamond and Carbon-based Materials Research · Metal and Thin Film Mechanics · Advanced materials and composites

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (15)

Show source-provided references
1. Robertson · Mater. Sci. Eng., R Rep. · 2002 · 37 · 12910.1016/S0927-796X(02)00005-0 ↗
2. Grill · Surf. Coat. Technol. · 1997 · 94–95 · 50710.1016/S0257-8972(97)00458-1 ↗
3. Pei · Surf. Coat. Technol. · 2005 · 198 · 4410.1016/j.surfcoat.2004.10.106 ↗
4. Corbella · Thin Solid Films · 2005 · 482 · 29310.1016/j.tsf.2004.11.178 ↗
5. Strondl · Surf. Coat. Technol. · 2003 · 162 · 28810.1016/S0257-8972(02)00497-8 ↗
6. Voevodin · Thin Solid Films · 1999 · 342 · 19410.1016/S0040-6090(98)01456-4 ↗
7. Palmquist · Thin Solid Films · 2003 · 444 · 2910.1016/S0040-6090(03)00937-4 ↗
8. Damasceno · Thin Solid Films · 2003 · 433 · 19910.1016/S0040-6090(03)00313-4 ↗
9. Vercammen · Tribol. Int. · 2004 · 37 · 98310.1016/j.triboint.2004.07.016 ↗
10. Fernandes · J. Mater. Res. · 2000 · 15 · 176610.1557/JMR.2000.0255 ↗
11. Antunes · Surf. Coat. Technol. · 2002 · 149 · 2710.1016/S0257-8972(01)01413-X ↗
12. ENV 1071-3 Advanced technical ceramics — methods of test for ceramic coatings: Part 3. Determination of adhesion and other mechanical failure modes by a scratch test, 2002.
13. Somekh · J. Vac. Sci. Technol., A · 1984 · 2 · 128510.1116/1.572396 ↗
14. Mattox · 1998
15. Lifshitz · Diamond Relat. Mater. · 1996 · 5 · 38810.1016/0925-9635(95)00445-9 ↗