Abstract
Abstract We have demonstrated that the surface recombination velocity can be lowered to as low as 1.3 cm/s for n-type c-Si wafers and to 9.0 cm/s for p-type wafers by using amorphous Si (a-Si) and Si nitride (SiNx) stacked films prepared by catalytic chemical vapor deposition (Cat-CVD). These values are much lower than those of c-Si wafers passivated by same stacked structures formed by low-damage remote plasma-enhanced CVD (PECVD). It is revealed that Cat-CVD a-Si insertion layers play an important role to improve interface quality, and also SiNx films are also essential for reducing the surface recombination velocity down to such low levels.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Semiconductor materials and devices · Thin-Film Transistor Technologies · Silicon and Solar Cell Technologies
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (10)
Show source-provided references
1. Larionova · Appl. Phys. Lett. · 2010 · 96 · 03210510.1063/1.3291681 ↗
2. Kerr · Semicond. Sci. Technol. · 2002 · 17 · 3510.1088/0268-1242/17/1/306 ↗
3. Hoex · J. Appl. Phys. · 2008 · 104 · 04490310.1063/1.2963707 ↗
4. Focsa · Mater. Sci. Eng. B. · 2009 · 159 · 24210.1016/j.mseb.2009.02.009 ↗
5. Matsumura · J. Appl. Phys. · 1989 · 65 · 439610.1063/1.343278 ↗
6. Jin · 2009 · 72
7. A. Kikkawa. H. Matsumura, (unpublished).
8. Aubert · 1998 · 283
9. Gielis · Thin Solid Films · 2009 · 517 · 345610.1016/j.tsf.2009.01.076 ↗
10. Matsumura · Phys. Status Solidi C · 2010 · 7 · 113210.1002/pssc.200982821 ↗