Microstructure and mechanical properties of as-deposited and annealed TiB2/BN superlattice coatings
Source abstract
Abstract
Abstract TiB 2 /BN multilayers with the modulation ratios ( t TiB2 :t BN ) ranging from 1:1 to 16:1 and a constant modulation period of 24 nm were prepared by magnetron sputtering. The TiB 2 /BN multilayers were subsequently annealed in a vacuum environment at temperatures of 500–700 °C for 30 min, then characterized by extensive measurements. All multilayers exhibited small grain sizes and stable layer structures with polycrystalline with TiB 2 (001), TiB 2 (101), TiB 2 (002) textures or amorphous BN, resulting in higher hardness and elastic modulus than that of individual monolithic TiB 2 or BN coatings. The hardness of as-deposited multilayer can reach as high as 39.34 GPa at t TiB2 :t BN = 13:1, meanwhile the friction coefficient got to 0.028, which was also the lowest. The hardness and friction were almost unchanged after annealing at 500–700 °C, which was attributed to good thermal stability in the layer structure and the existence of stable TiB x N y phases.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Metal and Thin Film Mechanics · Diamond and Carbon-based Materials Research · Boron and Carbon Nanomaterials Research
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References
Reference metadata was not supplied for this record.