Effects of annealing on the crystallization and roughness of PLZT thin films
Source abstract
Abstract
Abstract Lead lanthanum zirconate titanate (PLZT) thin films with stoichiometry (9/65/35) were prepared by a dip-coating process using a polymeric organic solution. The solution viscosity was adjusted in the range of 15–56 cP. Silicon (100) substrates were previously cleaned and then immersed in the solution. The withdrawal speed of substrate from the solution was adjusted within a range of 5–20 mm/min. The coated substrates were thermally treated in the 450–700°C temperature range. Surface roughness and crystallization of these films are strongly dependent on the annealing conditions. Infrared and X-ray diffraction data for PLZT powders heat-treated at 650°C for 3 h show that the material is free of carbonate phases and crystalline.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Ferroelectric and Piezoelectric Materials · Photorefractive and Nonlinear Optics · Acoustic Wave Resonator Technologies
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References
Reference metadata was not supplied for this record.