Substrate and coating defect planarization strategies for high-laser-fluence multilayer mirrors
Source abstract
Abstract
Abstract Planarizing or smoothing over nodular defects in multilayer mirrors can be accomplished by a discrete deposit-and-etch process that exploits the angle-dependent etching rate of optical materials. Typically, nodular defects limit the fluence on mirrors irradiated at 1064 nm with 10 ns pulse lengths due to geometrically- and interference-induced light intensification. Planarized hafina/silica multilayer mirrors have demonstrated > 125 J/cm2 laser resistance for single-shot testing and 50 J/cm2 for multi-shot testing for nodular defects originating on the substrate surface. Two planarization methods were explored: thick planarization layers on the substrate surface and planarized silica layers throughout the multilayer in which only the silica layers that are below one half of the incoming electric field value are etched. This paper also describes the impact of planarized defects that are buried within the multilayer structure compared to planarized substrate particulate defects.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Laser Material Processing Techniques · Solid State Laser Technologies · Advanced Optical Sensing Technologies
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References
Reference metadata was not supplied for this record.