Abstract
Abstract Polycrystalline titanium thin films have been widely employed as interlayer between the substrate and different coatings in order to improve adhesion strength, corrosion resistance and wear performance, as well as to promote the growth of crystalline phases of the coating. The thickness of the Ti layer can be relevant on the behavior of the coatings, however very few studies have been carried out. In this work, the crystal structure of polycrystalline titanium films deposited with a vacuum arc discharge on monocrystalline silicon wafers (100) was studied and a dependence on the film thickness was found. The presence of the fcc phase of titanium was observed for the thinnest films with a critical thickness estimated in 300 nm, a much larger value than those reported for other deposition processes. For larger thicknesses, the films grew as α-titanium with a preferred orientation in the [100] direction. The obtained results agreed with a growth model based on the matching between the film and the substrate lattice. The characteristics of the films deposited in two steps, which had not been previously investigated, reinforced the suggested model.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Metal and Thin Film Mechanics · Copper Interconnects and Reliability · High-Temperature Coating Behaviors
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (17)
Show source-provided references
1. Titanium interlayer to improve the adhesion of multilayer amorphous boron carbide coating on silicon substrate10.1016/j.apsusc.2012.11.123 ↗
2. Growth and characteristics of diamond-like carbon films with titanium and titanium nitride functional layers by cathode arc plasma10.1016/j.surfcoat.2013.02.020 ↗
3. Magnetron sputtered TiO2 films on a stainless steel substrate: selective rutile phase formation and its tribological and anti-corrosion performance10.1016/j.tsf.2011.01.042 ↗
4. Pressure-induced α→ωα→ω transition in titanium metal: a systematic study of the effects of uniaxial stress10.1016/j.physb.2004.10.030 ↗
5. Epitaxial growth of titanium thin films10.1116/1.1315691 ↗
6. Epitaxial growth of fcc Ti films on Al(001) surfaces10.1103/PhysRevB.56.9841 ↗
7. Growth of face-centred-cubic titanium on aluminium
8. Interface structure of face-centered-cubic-Ti thin film grown on 6H–SiC substrate10.1557/JMR.2000.0305 ↗
9. Thickness-dependence fcc–hcp phase transformation in polycrystalline titanium thin films10.1016/j.actamat.2010.12.046 ↗
10. X-Ray reflectivity analysis of titanium dioxide thin films grown by cathodic arc deposition10.1166/jnn.2014.8017 ↗
11. X-ray and neutron scattering from rough surfaces10.1103/PhysRevB.38.2297 ↗
12. Elastic stability and electronic structure of fcc Ti, Zr, and Hf: a first-principles study10.1103/PhysRevB.65.092106 ↗
13. Scherrer after sixty years: a survey and some new results in the determination of crystallite size10.1107/S0021889878012844 ↗
14. Stress and microstructure of sputter-deposited thin films: molecular dynamics investigations10.1063/1.339559 ↗
15. Mechanical properties of thin films10.1007/BF02666659 ↗
16. Identification of metastable phases: face-centred cubic Ti10.1088/0953-8984/9/29/009 ↗
17. The formation of f.c.c. titanium in titanium-aluminium multilayers10.1016/1359-6454(95)00159-5 ↗