Comparison of microstructure and phase transformation for nanolayered CrN/AlN and TiN/AlN coatings at elevated temperatures in air environment
Source abstract
Abstract
CrN/AIN and TiN/AIN multilayer coatings with modulation period of 4 nm and thickness ratio equal to 1.0 were manufactured by RF magnetron sputtering. Both films were annealed at temperatures of 800 °C in air for 1 h and then for an additional 9 h. Both coatings in as-deposited and after heat treatment were evaluated with a transmission electron microscope (TEM) equipped with EDS. After heat treatment at 800 °C for 1 h, a thick oxide layer around 260 nm was formed on the surface of the TiN/AIN coating. The oxide layer which formed on the coating was composed of three different regimes, including Al-enriched oxide with excess oxygen on the top surface, a crystalline Al-depleted TiO 2 layer 30-80 nm thick above the nitride coating and in between, mixed nano-crystalline Al 2 O 3 and TiO 2 films. In comparison, only one oxide layer smaller than 50 nm in thickness was found in the annealed CrN/AIN coating. This amorphous or nanocrystalline oxide layer identified by EDS was a metal-deficient oxide, in which Al 2 O 3 and Cr 2 O 3 were mixed together forming a solid solution. As a result, the CrN/AIN coating exhibited superior stability compared to the TiN/AIN coating at elevated temperatures.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Metal and Thin Film Mechanics · Diamond and Carbon-based Materials Research · GaN-based semiconductor devices and materials
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References
Reference metadata was not supplied for this record.