Effect of thermal annealing on the performance of WO 3 –Ag–WO 3 transparent conductive film
Source abstract
Abstract
Abstract As a candidate for transparent electrodes, oxide–metal–oxide tri-layer films have attracted a lot of interest by virtue of their low cost and decent performance. However, their thermal stability needs to be considered before device integration. Here, we report a thermal annealing effect on the performance of WO 3 –Ag–WO 3 (WAW) transparent conductive thin film prepared by thermal evaporation. We find that the sheet resistance of the as-prepared WAW film gradually increases from 6.55 to 21.4 Ω/sq when the annealing temperature reaches 400 °C. With a low annealing temperature (below 200 °C), the luminous transmittance of the WAW film slightly increases but decreases rapidly when the annealing temperature exceeds 200 °C. The maximum figure of merit (11 × 10 − 3 Ω − 1 ) was obtained at the annealing temperature of 100 °C. Above the annealing temperature of 300 °C, the film shows significant transmittance and conductivity degradation, which can be attributed to the decrease of intrinsic dielectric constant of WO 3 layers and the reduction of connectivity between Ag islands upon high temperature annealing, respectively. Annealing at a temperature of 500 °C leads to severe destruction of the tri-layer structure. In addition, we believe that the localized surface plasmonic absorption of annealing-generated Ag nanoparticles results in a valley centered at 410 nm on the transmittance spectrum of the 500 °C annealed WAW film.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: ZnO doping and properties · Gas Sensing Nanomaterials and Sensors · Transition Metal Oxide Nanomaterials
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References
Reference metadata was not supplied for this record.