Effects of oxygen flow ratios and annealing temperatures on Raman and photoluminescence of titanium oxide thin films deposited by reactive magnetron sputtering
Source abstract
Abstract
Abstract Titanium oxide (TiO x ) thin films were deposited on the Si(100) substrates by direct-current reactive magnetron sputtering at 3–15 % oxygen flow ratios (FO 2 % = FO 2 /(FO 2 + FAr) × 100%), and then annealed by rapid thermal annealing (RTA) at 350–750 °C for 2 min in air. The phase, bonding and luminescence behaviors of the as-deposited and annealed TiO x thin films were analyzed by X-ray diffraction (XRD), Raman spectroscopy and photoluminescence (PL) spectroscopy, respectively. The as-deposited TiO x films were amorphous from XRD and showed weak Raman intensity. In contrast, the distinct crystalline peaks of anatase and rutile phases were detected after RTA at 550–750 °C from both XRD and Raman spectra. A mixture of anatase and rutile phases was obtained by RTA at 3 FO 2 % and its amount increased with annealing temperature. Only the anatase phase was detected in the 6–15 FO 2 % specimens after RTA. The PL spectra of all post-annealed TiO x films showed a broad peak in visible light region. The PL peak of TiO x film at 3 FO 2 % at 750 °C annealing can be fitted into two Gaussian peaks at ~ 486 nm (2.55 eV) and ~ 588 nm (2.11 eV) which were attributed to deep-level emissions of oxygen vacancies in the rutile and anatase phases, respectively. The peak around 550 nm was observed at 6–15 FO 2 % which is attributed to electron–hole pair recombination from oxygen vacancy state in anatase phase to valence band. The variation of intensity of PL peaks is concerned with the formation of the rutile and anatase phases at different FO 2 % and annealing temperatures.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: TiO2 Photocatalysis and Solar Cells · Advanced Photocatalysis Techniques · ZnO doping and properties
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (22)
Show source-provided references
1. O'Regan · Nature · 1991 · 353 · 73710.1038/353737a0 ↗
2. Masaaki · Appl. Catal. A Gen · 2007 · 325 · 110.1016/j.apcata.2007.03.013 ↗
3. Al-Homoudi · Appl. Surf. Sci. · 2007 · 253 · 860710.1016/j.apsusc.2007.04.068 ↗
4. San Vicente · Thin Solid Films · 2002 · 403–404 · 33510.1016/S0040-6090(01)01572-3 ↗
5. Pomoni · J. Non-Cryst. Solids · 2008 · 354 · 444810.1016/j.jnoncrysol.2008.06.069 ↗
6. Natarajan · Thin Solid Films · 1998 · 322 · 610.1016/S0040-6090(97)01010-9 ↗
7. Masahiro · Appl. Surf. Sci. · 2001 · 169–170 · 535
8. Lianchao · Thin Solid Films · 2004 · 455–456 · 525
9. Hongfu · J. Non-Cryst. Solids · 2008 · 354 · 144010.1016/j.jnoncrysol.2007.01.108 ↗
10. Boukrouh · Thin Solid Films · 2008 · 516 · 635310.1016/j.tsf.2007.12.150 ↗
11. GoHmez · Sol. Energy Mater. Sol. Cells · 2000 · 64 · 38510.1016/S0927-0248(00)00231-2 ↗
12. Terufumi · Mater. Chem. Phys. · 2008 · 111 · 48610.1016/j.matchemphys.2008.04.053 ↗
13. Tang · J. Appl. Phys. · 1994 · 75 · 204210.1063/1.356306 ↗
14. Sekiya · J. Lumin. · 2000 · 87–89 · 114010.1016/S0022-2313(99)00570-0 ↗
15. Koji · J. Lumin. · 2008 · 128 · 91110.1016/j.jlumin.2007.11.071 ↗
16. Baoshun · Mater. Chem. Phys. · 2007 · 106 · 35010.1016/j.matchemphys.2007.06.012 ↗
17. Campuzano · J. Phys. Chem. Solids · 2001 · 62 · 3510.1016/S0022-3697(00)00097-4 ↗
18. Ke-Rong · Phys. Lett. A · 2005 · 340 · 22010.1016/j.physleta.2005.04.008 ↗
19. Gr¨azel · 1989
20. Sze · 2002
21. Livraghi · J. Am. Chem. Soc. · 2006 · 128 · 1566610.1021/ja064164c ↗
22. Henderson · J. Phys. Chem. B · 2003 · 107 · 53410.1021/jp0262113 ↗