Deposition of B4C/BCN/c-BN multilayered thin films by r.f. magnetron sputtering

G. Bejarano, J.M. Caicedo, E. Baca, P. Prieto, A.G. Balogh, S. Enders

Thin Solid Films· Volume 494· Issue 1-2
Publisher page

Abstract

Thin films of cubic boron nitride (c-BN) and B4C/BCN/c-BN multilayers, were deposited by r.f. (13.56 MHz) multi-target magnetron sputtering from high-purity (99.99%) h-BN and a (99.5%) B4C targets, in an Ar (90%)/N2 (10%) gas mixture. Films were deposited onto silicon substrates with (100) orientations at 300 °C, with r.f. power density near 7 W/cm2. In order to obtain the highest fraction of the c-BN phase, an r.f. substrate bias voltage between − 100 and − 300 V was applied during the initial nucleation process and − 50 to − 100 V during the film growth. Additionally, B4C and BCN films were deposited and analyzed individually. For their deposition, we varied the bias voltage of the B4C films between − 50 and − 250 V, and for the BCN coatings, the nitrogen gas flow from 3% to 12%. A 300-nm-thick TiN buffer layer was first deposited to improve the adhesion of all samples. X-ray diffraction patterns revealed the presence of c-BN (111) and h-BN phases. FTIR spectroscopy measurements indicate the presence of a peak at 780 cm− 1 referred to as “out-of-plane” h-BN vibration mode; another peak at 1100 cm− 1 corresponds to the c-BN TO mode and the “in-plane” vibration mode of the h-BN at 1400 cm− 1. BN films deposited at 300 °C at a pressure of 4.0 Pa and under − 150 V of nucleation r.f. bias, applied for 35 min, presented the highest c-BN fraction, near 85%. By using 32 layers, it was possible to deposit a 4.6-μm-thick c-BN film with adequate mechanical properties and good adhesion to the substrate.
Source: expertdata · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Metal and Thin Film Mechanics · Boron and Carbon Nanomaterials Research · Diamond and Carbon-based Materials Research

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (14)

Show source-provided references
1. Vel · Mater. Sci. Eng., B · 1991 · 10 · 14910.1016/0921-5107(91)90121-B ↗
2. Demazeau · Diamond Relat. Mater. · 1993 · 2 · 19710.1016/0925-9635(93)90052-4 ↗
3. Zhang · MRS Bull./March · 2003 · 18410.1557/mrs2003.60 ↗
4. Ulrich · Surf. Coat. Technol. · 1999 · 116–119 · 26910.1016/S0257-8972(99)00396-5 ↗
5. Yamamoto · Surf. Coat. Technol. · 2001 · 142–144 · 88110.1016/S0257-8972(01)01212-9 ↗
6. Kidner · Appl. Phys. Lett. · 1994 · 64 · 1410.1063/1.111779 ↗
7. Klepper · Fus. Technol. · 2001 · 39 · 91010.13182/FST01-A11963356 ↗
8. Lee · Phys. Status Solidi B · 2004 · 241 · 163710.1002/pssb.200304574 ↗
9. Chung I. Chiang, Research Report FZKA 5644 1995, Research Centre Karlsruhe, Germany.
10. T. Eckardt, K. Bewilogua, G. van der Kolk, T. Hurkmans, T. Trinh, W. Fleischerb, Technical Report of Hauser Techno Coating Europe BV, 2000, Hauzer Techno Coating Europe BV, Groethofstraat 22 b, NL-5916 PB Venlo, The Netherlands.
11. Cao · J. Vac. Sci. Technol., B · 2002 · 2010.1116/1.1518973 ↗
12. Marshall · J. Am. Ceram. Soc. · 1979 · 69 · 347
13. National Institute of Standards and Technology of USA 01/10/2000.
14. Yamamoto · Thin Solid Films · 2000 · 377–378 · 33110.1016/S0040-6090(00)01364-X ↗