Composition dependent thermoelectric properties of sintered Mg2Si1−Ge (x= 0 to 1) initiated from a melt-grown polycrystalline source
Source abstract
Abstract
Fabrication of Mg 2 Si 1-x Ge x (x=0-1.0) was carried out using a spark plasma sintering technique initiated from melt-grown polycrystalline Mg 2 Si 1-x Ge x powder. The thermoelectric properties were evaluated from RT to 873 K. The power factor of Mg 2 Si 1-x Ge x with higher Ge content (x=0.6-1.0) tends to decrease at higher temperatures, and the maximum value of about 2.2 x 10 -5 Wcm -1 K -2 was observed at 420 K for Mg 2 Si and Mg 2 Si 0.6 Ge 0.4 . The coexistence of Si and Ge gave rise to a decrease in the thermal conductivity in the Mg 2 Si 1-x Ge x . The values close to 0.02 Wem -1 K -1 were obtained for Mg 2 Si 1-x Ge x (ℵ= 0.4-0.6) over the temperature range from 573 to 773 K, with the minimum value being about 0.018 Wcm -1 K -l at 773 K for Mg 2 Si 0.4 Ge o-6 . The maximum dimensionless figure of merit was estimated to be 0.67 at 750 K for samples of Mg2Si 0. 6Ge 0.4 .
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Advanced Thermoelectric Materials and Devices · Thermal Expansion and Ionic Conductivity · Chalcogenide Semiconductor Thin Films
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References
Reference metadata was not supplied for this record.