Improvement of secondary electron emission property of MgO protective layer for an alternating current plasma display panel by addition of TiO2
Source abstract
Abstract
Abstract Secondary electron emission from a cathode material in an AC plasma display panel (PDP) is dominated by potential emission mechanism, which is sensitive to band structure of a protective layer. Therefore, the secondary electron emission property can be modified by a change in the energy band structure of the protective layer. Mg 2−2 x Ti x O 2 films were prepared by an e-beam evaporation method to be used as possible substitutes for the conventional MgO protective layer. The oxygen content in the films and in turn, the ratio of metal to oxygen gradually increased with increasing TiO 2 content in the starting materials. The stress relaxation, when the [TiO 2 /(MgO+TiO 2 )] ratio in the evaporation starting materials was 0.15, seems to be related to the rough surface grown by Stranski–Krastanov mode due to the poor lattice matching condition between substrate and film. The film density, which was calculated from the refractive index, had a maximum at the [TiO 2 /(MgO+TiO 2 )] ratio of 0.15 and then gradually decreased with a further increase in the [TiO 2 /(MgO+TiO 2 )] ratio in the starting materials. When the [TiO 2 /(MgO+TiO 2 )] ratios of 0.1 and 0.15 were used, the deposited films exhibited the secondary electron emission yields improved by 50% compared to that of the conventional MgO protective layer.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Plasma Diagnostics and Applications · ZnO doping and properties · GaN-based semiconductor devices and materials
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References
Reference metadata was not supplied for this record.