Electro-optical and structural properties of thin ZnO films, prepared by filtered vacuum arc deposition
Source abstract
Abstract
Abstract Thin ZnO films were deposited at room temperature on glass substrates by a filtered vacuum arc deposition system. The electrical, optical and structural properties were investigated as a function of the oxygen pressure in the range of 0.26–0.73 Pa and arc current in the range of 100–300 A. No additional treatment was applied to the samples. Film thickness was in the range of 100–400 nm, depending linearly on the arc current. As-deposited electrical resistivity was in the range of (1–2)×10−4 Ω m and the optical transmission of 300-nm-thick films was in the range of 85–95% in the visible and near-IR spectral region. Minimal resistivity of 1.05×10−4 Ω m was obtained for a 240-nm-thick film, which had ∼94% transmittance in the visible and near-IR range, and which was deposited at 0.42-Pa oxygen pressure. The relative standard deviation of the measured parameters, determined on a set of seven samples deposited with the same current and pressure was less than 4%. XPS analysis showed that the films were non-stoichiometric both on the surface and within the film, and that the composition was weakly pressure dependent. X-ray diffraction analysis showed the films to be crystalline, with a pressure dependent preferred orientation.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: ZnO doping and properties · Gas Sensing Nanomaterials and Sensors · Copper-based nanomaterials and applications
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References
Reference metadata was not supplied for this record.