Temperature dependence of Fluorine-doped tin oxide films produced by ultrasonic spray pyrolysis
Source abstract
Abstract
Abstract Fluorine-doped tin oxide (FTO) films were prepared at different substrate temperatures by ultrasonic spray pyrolysis technique on glass substrates. Among F-doped tin oxide films, the lowest resistivitiy was found to be 6.2 × 10− 4 Ω-cm for a doping percentage of 50 mol% of fluorine in 0.5 M solution, deposited at 400 °C. Hall coefficient analyses and secondary ion mass spectrometry (SIMS) measured the electron carrier concentration that varies from 3.52 × 1020 cm− 3 to 6.21 × 1020 cm− 3 with increasing fluorine content from 4.6 × 1020 cm− 3 to 7.2 × 1020 cm− 3 in FTO films deposited on various temperatures. Deposition temperature on FTO films has been optimized for achieving a minimum resistivity and maximum optical transmittance.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: ZnO doping and properties · Ga2O3 and related materials · Gas Sensing Nanomaterials and Sensors
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (9)
Show source-provided references
1. Colen · Thin Solid Films · 1981 · 77 · 12710.1016/0040-6090(81)90367-9 ↗
2. Patil · Thin Solid Films · 2003 · 437 · 3410.1016/S0040-6090(03)00680-1 ↗
3. Dima · Thin Solid Films · 2003 · 427 · 42710.1016/S0040-6090(02)01217-8 ↗
4. Lee · Thin Solid Films · 2002 · 416 · 27110.1016/S0040-6090(02)00619-3 ↗
5. Kane · J. Electrochem. Soc. · 1976 · 123 · 27010.1149/1.2132802 ↗
6. Blanton · Mater. Res. Bull. · 1994 · 29 · 53710.1016/0025-5408(94)90043-4 ↗
7. Rajpure · Mater. Chem. Phys. · 2000 · 64 · 18410.1016/S0254-0584(99)00256-4 ↗
8. Patil · Mater Chem Phys. · 1999 · 59 · 15810.1016/S0254-0584(99)00049-8 ↗
9. Elangovan · J. Optoelect. Adv. Mater. · 2003 · 5 · 45