article·2005-04-22

Optical properties and surface morphology of evaporated (WO3)1−x–(Fe2O3)x thin films

Alireza Z. Moshfegh, R. Azimirad, Omid Akhavan

Publisher page

Abstract

Abstract Thin films of (WO 3 ) 1 − x –(Fe 2 O 3 ) x composition were deposited by thermal evaporation on glass substrates and then all samples were annealed at 400 °C in air. Optical properties such as transmittance, reflectance, and optical bandgap energy of the “as deposited” and the annealed films were studied using ultraviolet–visible spectrophotometry. It was shown that the annealing process did not substantially change the optical transmittance and reflectance of all the films except the films having x = 0.75. By increasing Fe 2 O 3 content in the films from x = 0 to x = 0.75, optical bandgap energy decreased from 3.4 to about 1.3 eV and from 3.1 to 2.1 eV for the “as deposited” and the annealed samples, respectively. Moreover, using X-ray photoelectron spectroscopy, we have shown that the “as deposited” (WO 3 ) 0.25 –(Fe 2 O 3 ) 0.75 films contained Fe 3 O 4 , and it converted to Fe 2 O 3 after the annealing process. Using atomic force microscopy, it was found that the grain size and surface roughness of the annealed films were greater than the “as deposited” ones. In addition, for the annealed films with intermediate x 's, we have observed a smoother surface with smaller grain size as compared to films with the other x 's.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Transition Metal Oxide Nanomaterials · Gas Sensing Nanomaterials and Sensors · Analytical Chemistry and Sensors

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.