Indium–tin-oxide thin films prepared by dip-coating of indium diacetate monohydroxide and tin dichloride
Source abstract
Abstract
Abstract Tin-doped In 2 O 3 (ITO) films were prepared by the dip-coating method using an ethanol solution of indium diacetate monohydroxide, In(OH)(CH 3 COO) 2 , and tin dichloride, SnCl 2 ·2H 2 O, with 2-aminoethanol (monoethanolamine), H 2 NC 2 H 4 OH. The influence of the tin concentration was investigated between 0 and 20 at.% Sn. The composition of the films (thickness ∼90 nm) approximately agreed with that of the solution when the dipping and the heating at 600°C in air for 30 min were repeated three times. The lattice constant of the ITO films increased by the tin addition and annealing at 600°C for 1 h in a nitrogen flow. The films were highly transparent in the visible range. At 6.4 at.% Sn, the maximum carrier concentration (6.2×10 20 cm −3 ) and minimum resistivity (5.8×10 −4 Ω cm) were obtained after annealing in nitrogen (oxygen partial pressure ∼2.0 Pa). The mobilities of the ITO films (∼10 cm 2 V −1 s −1 ) were almost independent of the film composition and the annealing. The mobilities of the undoped In 2 O 3 films were ∼40 cm 2 V −1 s −1 .
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: ZnO doping and properties · Gas Sensing Nanomaterials and Sensors · Transition Metal Oxide Nanomaterials
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References
Reference metadata was not supplied for this record.