Composition, structure, microhardness and residual stress of W–Ti–N films deposited by reactive magnetron sputtering
Source abstract
Abstract
Abstract W–Ti–N films were deposited by reactive DC magnetron sputtering from a W–Ti (30 at.%) target, in a mixture of argon and nitrogen at a total pressure of 0.5 Pa, onto steel and silicon substrates. The crystal structure, microstructure, composition, micro-hardness and residual stress were studied as a function of the partial pressure of nitrogen. Films containing less than 30 at.% nitrogen were composed of a mixture of b.c.c. W and f.c.c. W 2 N phases, while only the f.c.c. phase, probably W x Ti 1− x N y , was present in the films with a nitrogen concentration of [N]≥36 at.%. The microhardness of the W–Ti–N films increased with increasing nitrogen concentration from 25 GPa for [N]=0 up to a maximum of approximately 65 GPa at [N]=25 at.%. This was accompanied by increasing microstrain, while the compressive residual stress remained in the range of 1.3–2.3 GPa. The single-phase W–Ti–N films, with [N]≥36 at.%, exhibited a micro-hardness of approximately 40 GPa and a large compressive stress of, at most, approximately 5.7 GPa at [N]=40 at.%. The maximum microhardness was found in films that simultaneously possessed: (i) the presence of two crystalline phases; (ii) large microstrain; and (iii) relatively low compressive residual stress.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Metal and Thin Film Mechanics · Diamond and Carbon-based Materials Research · Semiconductor materials and devices
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References
Reference metadata was not supplied for this record.