Contact damage in TiN coatings on steel

S. Bhowmick, A. Kale, Vikram Jayaram, S.K. Biswas

Publisher page

Abstract

Damage mechanisms beneath Vickers indentations are examined on 5\mu m TiN film deposited on stainless steel substrate as a function of load. Prominent mode of cracking includes surface edge cracks and subsurface inclined cracks. No interfacial delaminations were noted at the TiN/steel interface. The tangential traction, radial stress and shear stress distribution around an axisymmetric indentation field are used to assess the driving force for crack propagation.