Growth and structural characterization of yttria-stabilized zirconia–gold nanocomposite films with improved toughness
Source abstract
Abstract
Abstract To counteract the natural brittleness of oxide ceramic films and achieve better toughness, nanocomposite films combining yttria-stabilized zirconia (YSZ) and gold were produced. A hybrid of magnetron sputtering and pulsed laser ablation was used to grow crystalline YSZ embedded in an amorphous YSZ/Au matrix at near room temperature. Results from chemical analyses, X-ray and electron diffraction, high-resolution transmission electron microscopy, lateral force microscopy, nanoindentation hardness measurements and toughness estimates are discussed. At a fixed deposition temperature, the film microstructure was critically dependent on the gold content. Three distinct microstructures were produced: an amorphous YSZ/Au coating at less than 8 at.% Au; 5–10 nm YSZ crystals embedded in an amorphous YSZ/Au matrix at 10–15 at.% Au; and 20–100-nm crystallites of (101)-oriented YSZ mixed with micron-sized Au agglomerates at above 20 at.% Au. From these films, only the 5–10 nm nanocrystalline YSZ embedded in the amorphous YSZ/Au matrix provided the improvements in toughness. Coatings with this structure had hardness of 15–20 GPa, elastic modulus of approximately 250 GPa, and did not develop cracks in Vickers pyramid indentation at loads up to 1 kg, showing remarkable ductility. The improvement in toughness of this relatively hard film was explained by grain boundary sliding of YSZ nanocrystals in the YSZ/Au amorphous matrix. The new YSZ/Au nanocomposite films developed in this study may have good potential for surface protection, where a combination of thermal stability, oxidation resistance and improved film toughness are required.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Metal and Thin Film Mechanics · Electronic and Structural Properties of Oxides · Advanced materials and composites
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (45)
Show source-provided references
1. Chiang · 1997
2. Wachtman · 1996
3. Ganapathi · IEEE Trans. Magn. · 1992 · 28 · 253310.1109/20.179547 ↗
4. Moulzolf · Thin Solid Films · 1999 · 347 · 22010.1016/S0040-6090(99)00046-2 ↗
5. Yamashita · IEEE Trans. Magn. · 1988 · 24 · 262910.1109/20.92195 ↗
6. Kao · J. Vac. Sci. Technol. A · 1990 · 8 · 328910.1116/1.576580 ↗
7. Dugger · Tribol. Trans. · 1993 · 36 · 8410.1080/10402009308983136 ↗
8. Theunissen · J. Mater. Sci. Lett. · 1998 · 17 · 123510.1023/A:1006518500055 ↗
9. Miller · J. Appl. Phys. · 1990 · 67 · 487210.1063/1.344763 ↗
10. Dai · J. Mater. Res. · 1999 · 14 · 132910.1557/JMR.1999.0181 ↗
11. Delgado · Appl. Phys. Lett. · 1996 · 68 · 104810.1063/1.116244 ↗
12. Yang · Physica C · 1998 · 307 · 8710.1016/S0921-4534(98)00419-5 ↗
13. Voevodin · Appl. Phys. Lett. · 2001 · 78 · 73010.1063/1.1345823 ↗
14. Voevodin · J. Vac. Sci. Technol. A · 2001 · 19 · 132010.1116/1.1355360 ↗
15. Voevodin · J. Appl. Phys. · 2000 · 88 · 108810.1063/1.373781 ↗
16. Vepřek · J. Vac. Sci. Technol. A · 1999 · 17 · 240110.1116/1.581977 ↗
17. Hauert · Adv. Eng. Mater. · 2000 · 2 · 24710.1002/(SICI)1527-2648(200005)2:5<247::AID-ADEM247>3.0.CO;2-U ↗
18. Musil · Surf. Coat. Technol. · 2000 · 125 · 32210.1016/S0257-8972(99)00586-1 ↗
19. Voevodin · Thin Solid Films · 2000 · 370 · 22310.1016/S0040-6090(00)00917-2 ↗
20. Voevodin · J. Mater. Sci. · 1998 · 33 · 31910.1023/A:1004307426887 ↗
21. Fusaro · Lubr. Eng. · 1995 · 51 · 182
22. Spalvins · Thin Solid Films · 1978 · 53 · 28510.1016/0040-6090(78)90222-5 ↗
23. Voevodin · Appl. Phys. Lett. · 1996 · 69 · 18810.1063/1.117367 ↗
24. Voevodin · Thin Solid Films · 1999 · 342 · 19410.1016/S0040-6090(98)01456-4 ↗
25. Voevodin · J. Vac. Sci. Technol. A · 1999 · 17 · 98610.1116/1.581674 ↗
26. Voevodin · Surf. Coat. Technol. · 1999 · 116–119 · 3610.1016/S0257-8972(99)00228-5 ↗
27. Voevodin · J. Appl. Phys. · 1997 · 82 · 85510.1063/1.365784 ↗
28. JCPDS Powder Diffraction File, International Center for Powder Diffraction Data, Swarthmore, PA, 1998, Card 04-0784.
29. JCPDS Powder Diffraction File, International Center for Powder Diffraction Data, Swarthmore, PA, 1998, Card 17-0923.
30. JCPDS Powder Diffraction File, International Center for Powder Diffraction Data, Swarthmore, PA, 1998, Card 42-1164.
31. Meyer · Appl. Phys. Lett. · 1990 · 57 · 208910.1063/1.103950 ↗
32. Mate · Phys. Rev. Lett. · 1987 · 59 · 194210.1103/PhysRevLett.59.1942 ↗
33. Oliver · J. Mater. Res. · 1992 · 7 · 156410.1557/JMR.1992.1564 ↗
34. Cerny · Surf. Coat. Technol. · 1994 · 64 · 11110.1016/S0257-8972(09)90011-1 ↗
35. Greene · Appl. Phys. Lett. · 1995 · 67 · 292810.1063/1.114845 ↗
36. Adibi · J. Appl. Phys. · 1993 · 73 · 858010.1063/1.353388 ↗
37. Petrov · Appl. Phys. Lett. · 1993 · 63 · 3610.1063/1.109742 ↗
38. Hultman · J. Vac. Sci. Technol. A · 1991 · 9 · 43410.1116/1.577428 ↗
39. Mitterer · Z. Metallkd. · 1999 · 90 · 602
40. Tamayo · Appl. Phys. Lett. · 1996 · 68 · 229710.1063/1.116169 ↗
41. Liu · Wear · 1996 · 192 · 14110.1016/0043-1648(95)06784-1 ↗
42. Schwarz · Phys. Rev. B · 1997 · 56 · 698710.1103/PhysRevB.56.6987 ↗
43. Polaszyk · Surf. Sci. · 1998 · 402–404 · 45410.1016/S0039-6028(98)00033-8 ↗
44. Tanaka · J. Mater. Sci. · 1987 · 22 · 150110.1007/BF01233154 ↗
45. Voevodin · Surf. Coat. Technol. · 2001 · 146/147 · 35110.1016/S0257-8972(01)01396-2 ↗