article·2025-01-18Open access

Microstructure evolution of forsterite film during the high-temperature annealing process in grain-oriented silicon steel

Chengfu Han, Xianhui Wang, Ruifeng Li, Songshan Zhao, Jianhui Tian, Zhenyu Du, Fushan Li

Abstract

Forsterite films play an important role in enhancing the adhesion of the insulation layer and the magnetic properties of grain-oriented silicon steel. To clarify the microstructure evolution of forsterite film, an experiment involving high-temperature annealing at different temperatures ranging from 850 °C to 1150 °C was performed. Additionally, the reaction processes between MgO and the oxides formed in the decarburization oxide layer, such as SiO 2 and Fe 2 SiO 4 , were investigated. The initial formation temperature of the forsterite film is found to be within the range of 900 °C – 950 °C. The composition analysis reveals a decrease in the magnesium content from the surface toward the interior of the oxide layer. Up to 1100 °C, there is no longer a transition region between MgO and Fe 2 SiO 4 in the uppermost oxide layer, showing that the surface of oxide layer is composed entirely of forsterite. Simultaneously, with the diffusion of Mg 2+ , SiO 2 in the subsurface region reacts with Mg 2+ and is thus transformed into forsterite. The enrichment of aluminum, silicon, and oxygen in the bottom part of the oxide layer at 1100 °C implies the potential formation of mullite. These findings provide valuable insights to tune and control the forsterite film in grain-oriented silicon steel.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Microstructure and Mechanical Properties of Steels · Magnetic Properties and Applications · Metal Alloys Wear and Properties

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References

Reference metadata was not supplied for this record.