article·2008-08-14

Ex-situ wet clean and in-situ hydrogen clean for Si and SiGe epitaxy

T. Kormann, Philippe Garnier, G. Chabanne, A.W. Fortuin

Publisher page

Abstract

Abstract We report the comparison between two wet cleaning tools used for “HF-last” before epitaxy. The batch tool is more efficient in removing SiO 2 than the Single Wafer tool. We also show that a longer HF dispense time and a lower HF concentration are preferable. Then we saw that an in-situ H 2 bake before epitaxy is mandatory for a low defect epitaxy (0.08 defects cm − 2 ). SIMS profiles revealed that increasing the temperature and decreasing the pressure helps to get rid of Oxygen at the growth interface. A 775 °C H 2 bake at 20 Torr for 1 min is a minimum to reach a high quality epitaxy.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Semiconductor materials and devices · Advancements in Semiconductor Devices and Circuit Design · Thin-Film Transistor Technologies

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References

Reference metadata was not supplied for this record.