article·2015-08-01

Enhanced active P doping by using high order Ge precursors leading to intense photoluminescence

Yosuke Shimura, Srinivasan Ashwyn Srinivasan, Dries Van Thourhout, Rik Van Deun, Marianna Pantouvaki, Joris Van Campenhout, Roger Loo

Publisher page

Abstract

Abstract The impact of the growth temperature on the in-situ phosphorus doped Ge layer grown by chemical vapor deposition is studied to achieve a sufficiently high n-type carrier concentration for the realization of the quasi-direct band gap material in Ge. The use of a high order precursor gas, namely Ge2H6, allows to reduce the growth temperature down to 320 °C without degrading the material quality in view of optical applications. An active phosphorus concentration as high as 6.2 × 1019/cm3 has been measured by Hall effect measurements. The achieved active phosphorus concentration is the highest among the reported concentrations for uniformly in-situ doped Ge layers. The high and almost fully (87%) activated phosphorus concentration results in a strong photoluminescence peak at room temperature, which intensity is 8.3 times higher compared to the photoluminescence intensity as measured for an undoped Ge layer.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Photonic and Optical Devices · Semiconductor Quantum Structures and Devices · Nanowire Synthesis and Applications

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References

Reference metadata was not supplied for this record.