Comparison of thermal stability and combustibility between PI and PPS needle punched fabrics

Xiaoning Jiao

Abstract

Thermal analysis,limited oxygen index and cone calorimetry were used to compare the thermal stability and combustibility between polyimide(PI) and polyphenylene sulfide(PPS) needle punched fabrics.The results show that the decomposition temperature of PI and PPS needle punched fabrics is 580 ℃ and 500 ℃ respectively,LOI is 40% and 35%,ignition time is 38 s and 32 s,the maximum of heat release rate reaches 62.6 kW/m2 and 130.9 kW/m2,and the smoke factor is 12 MW/m2 and 35 MW/m2.By the comparison of these factors,a conclude that PI needle punched fabric is better than PPS in terms of thermal stability and combustibility is made.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Synthesis and properties of polymers · Flame retardant materials and properties · Epoxy Resin Curing Processes

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References

Reference metadata was not supplied for this record.