journal article·2016-01

Formation and properties of polypropylene/stearic acid composite fibers

Jan Broda, Czeslaw Slusarczyk, Janusz Fabia, Andrej Demsar

Textile Research Journal· Volume 86· Issue 1
Publisher page

Abstract

This paper refers to the formation and properties of polypropylene/stearic acid (PP/SA) composite fibers. For the investigation, commercial metallocene-catalyzed PP polymer and SA were used. The fibers were produced in laboratory conditions using the single screw spin draw device. The textile-mechanical properties, surface composition, morphology and supermolecular structure of as-spun fibers were studied. Moreover, the nonisothermal crystallization of the PP/SA blend and melting behavior of fibers were analyzed. In the investigation Fourier transform infrared–attenuated total reflectance, scanning electron microscopy, differential scanning calorimetry and wide-angle X-ray analytical methods were used. The research showed that the PP/SA blend has lower viscosity compared to the pure polymer and that during the PP crystallization phase, separation is induced. SA delays crystallization of PP, and interaction between SA and PP is observed. The as-spun PP/SA fibers have higher linear density, higher elongation at break and slightly lower tenacity compared to fibers produced from pure PP. The fibers contain a structure with high content of mesophase. During fiber formation, SA migrates towards the fiber surface and forms droplets located beneath the surface of the fiber or crystallizes outside in the form of flake-like crystals.
Source: crossref · Quality: baseline

Research context

OpenAlex topics: Polymer crystallization and properties · Fiber-reinforced polymer composites · Natural Fiber Reinforced Composites

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

Affiliations

University of Bielsko-Biala, Poland

University of Ljubjlana, Slovenia

References (37)

Show source-provided references
1. 10.1016/S0032-3861(03)00073-910.1016/S0032-3861(03)00073-9 ↗
2. 10.1002/app.2032710.1002/app.20327 ↗
3. 10.1016/S0079-6700(02)00002-310.1016/S0079-6700(02)00002-3 ↗
4. Everaert V · Chem Fibres Int · 2004 · 54 · 192
5. 10.1016/j.dyepig.2006.10.00410.1016/j.dyepig.2006.10.004 ↗
6. Broda J · Fibres Textil East Eur · 2007 · 15 · 30
7. 10.1016/0032-3861(70)90036-410.1016/0032-3861(70)90036-4 ↗
8. 10.1002/app.1988.07036050410.1002/app.1988.070360504 ↗
9. 10.1002/(SICI)1097-4628(19970516)64:7<1247::AID-APP1>3.0.CO;2-J10.1002/(SICI)1097-4628(19970516)64:7<1247::AID-APP1>3.0.CO;2-J ↗
10. 10.1002/app.1308310.1002/app.13083 ↗
11. 10.1002/pen.1082910.1002/pen.10829 ↗
12. 10.1002/app.1257010.1002/app.12570 ↗
13. 10.1021/cg049770310.1021/cg0497703 ↗
14. Demsar A · Tekstilec · 2000 · 43 · 398
15. Leskovsec M · Acta Chimica Slovenica · 2004 · 51 · 699
16. 10.1002/pen.2166510.1002/pen.21665 ↗
17. 10.1002/app.3105110.1002/app.31051 ↗
18. 10.1002/pen.2315310.1002/pen.23153 ↗
19. 10.1002/vnl.2010210.1002/vnl.20102 ↗
20. 10.1016/S0032-3861(02)00041-110.1016/S0032-3861(02)00041-1 ↗
21. Castro AJ. Methods for making microporous products . Patent 4 247498, USA, 1981.
22. 10.1016/0376-7388(91)80073-F10.1016/0376-7388(91)80073-F ↗
23. 10.1016/S0032-3861(98)00040-810.1016/S0032-3861(98)00040-8 ↗
24. 10.1016/0376-7388(95)00148-710.1016/0376-7388(95)00148-7 ↗
25. 10.1016/j.memsci.2010.11.01010.1016/j.memsci.2010.11.010 ↗
26. 10.1007/s00289005056510.1007/s002890050565 ↗
27. 10.1016/S0032-3861(02)00769-310.1016/S0032-3861(02)00769-3 ↗
28. 10.1002/app.2068610.1002/app.20686 ↗
29. 10.1016/j.eurpolymj.2006.01.00910.1016/j.eurpolymj.2006.01.009 ↗
30. 10.1515/POLYENG.2007.27.6-7.41110.1515/POLYENG.2007.27.6-7.411 ↗
31. 10.1002/app.3393110.1002/app.33931 ↗
32. Rabiej M · Fibres Textil East Eur · 2005 · 13 · 75
33. Rothon RN · 2003
34. Stuart B. Infrared spectroscopy: fundamentals and applications . Chichester: John Wiley & Sons, 2005.
35. Smith BC · 1996
36. 10.1016/0079-6700(91)90023-E10.1016/0079-6700(91)90023-E ↗
37. Broda J · Fibres Textil East Eur · 2003 · 11 · 95