journal article·2014-11

Preparation of quaternary ammonium salt of chitosan nanoparticles and their textile properties on Antheraea pernyi silk modification

Yanhua Lu, Dehong Cheng, Sheng Lu, Fengyuan Huang, Gang Li

Textile Research Journal· Volume 84· Issue 19
Publisher page

Abstract

A novel eco-friendly finishing agent of quaternary chitosan nanoparticles was prepared in two steps from a chitosan with low molecular weight. The water-soluble quaternary ammonium salt of chitosan, N-[(2-hydroxy-3-trimethylammonium)propyl] chitosan chloride (HTCC), was first synthesized in heterogeneous system by quaternization, and then HTCC was further prepared to nanoparticles via ionotropic gelation reaction in the presence of 1, 2, 3, 4-butane tetracarboxylic acid and sodium hypophosphite. The size distribution and morphology of the HTCC particles were characterized using a laser particle size analyzer and transmission electron microscope (TEM). When Antheraea pernyi ( A. pernyi) silk fabric was treated with HTCC nanoparticles by using a conventional dip-pad-dry-cure process, the modified A. pernyi silk fabric demonstrated durable wrinkle-resistant property, shrinkage-resistant property and antimicrobial activities against Staphylococcus aureus and Escherichia coli, even after being exposed to 50 consecutive home-laundering conditions. However, the modification of A. pernyi silk fabric caused breaking strength loss, breaking elongation reduction and initial modulus rise to some extent.
Source: crossref · Quality: baseline

Research context

OpenAlex topics: Silk-based biomaterials and applications · Nanocomposite Films for Food Packaging · Dyeing and Modifying Textile Fibers

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

Affiliations

Department of Light Chemical Engineering, Eastern Liaoning University, P. R. China

Institute of Applied Chemistry, Eastern Liaoning University, P. R. China

Experimental Center, Eastern Liaoning University, P. R. China

References (30)

Show source-provided references
1. Pascual E · J Bio Technol · 2001 · 8 · 289
2. 10.1016/j.polymer.2005.08.01910.1016/j.polymer.2005.08.019 ↗
3. 10.1177/004051751142660810.1177/0040517511426608 ↗
4. 10.1177/00405175030730121310.1177/004051750307301213 ↗
5. 10.1016/j.carbpol.2005.02.01910.1016/j.carbpol.2005.02.019 ↗
6. 10.1016/j.carbpol.2007.06.02710.1016/j.carbpol.2007.06.027 ↗
7. 10.1016/j.progpolymsci.2009.04.00110.1016/j.progpolymsci.2009.04.001 ↗
8. 10.1016/j.reactfunctpolym.2004.06.01010.1016/j.reactfunctpolym.2004.06.010 ↗
9. 10.1016/j.ijfoodmicro.2007.07.00310.1016/j.ijfoodmicro.2007.07.003 ↗
10. 10.1016/j.carbpol.2012.11.10010.1016/j.carbpol.2012.11.100 ↗
11. 10.1016/j.ijbiomac.2012.03.01810.1016/j.ijbiomac.2012.03.018 ↗
12. 10.1016/j.jcis.2011.02.05310.1016/j.jcis.2011.02.053 ↗
13. 10.1016/j.carbpol.2009.07.04510.1016/j.carbpol.2009.07.045 ↗
14. 10.1002/pi.305910.1002/pi.3059 ↗
15. 10.1016/S0142-9612(02)00507-010.1016/S0142-9612(02)00507-0 ↗
16. 10.1016/S0378-5173(02)00486-610.1016/S0378-5173(02)00486-6 ↗
17. Xu SF · J Wuhan U · 2004 · 50 · 721
18. Lu YH · J Appl Polym Sci · 2010 · 117 · 336210.1002/app.32094 ↗
19. 10.1016/j.lwt.2010.08.01810.1016/j.lwt.2010.08.018 ↗
20. 10.1016/j.carres.2003.10.02410.1016/j.carres.2003.10.024 ↗
21. 10.1177/004051751037626510.1177/0040517510376265 ↗
22. AATCC test method 124-2010. Smoothness appearance of fabrics after repeated home laundering.
23. AATCC Test Method 66-2008. Wrinkle recovery of woven fabrics: recovery angle.
24. AATCC Test Method 135-2012. Dimensional changes of fabrics after home laundering.
25. 10.1016/S0142-9612(99)00064-210.1016/S0142-9612(99)00064-2 ↗
26. 10.1016/S1381-5148(01)00111-010.1016/S1381-5148(01)00111-0 ↗
27. Xu YM · J Wuhan U · 2003 · 49 · 170
28. 10.1002/(SICI)1097-4628(19990718)73:3<363::AID-APP7>3.0.CO;2-R10.1002/(SICI)1097-4628(19990718)73:3<363::AID-APP7>3.0.CO;2-R ↗
29. 10.1177/00405175980680111210.1177/004051759806801112 ↗
30. 10.1108/RJTA-10-01-2006-B00610.1108/RJTA-10-01-2006-B006 ↗