Comparative study on the effects of superheated water and high temperature alkaline hydrolysis on wool keratin
Source abstract
Abstract
The purpose of this work is to understand the impact of superheated water hydrolysis treatment on the chemical properties of wool, and compare it with a conventional method of alkaline hydrolysis. The effects of hydrolysis temperature and concentration of alkali on the properties of wool were investigated. Superheated water hydrolysis was carried out at the temperatures of 140℃ and 170℃, with a material to liquor ratio of 1:3 for 1 hour. In conventional alkaline hydrolysis, the experiments were carried out in the same conditions using potassium hydroxide (KOH) and calcium oxide (CaO) with a concentration in the range of 5%–15% on the fiber weight (o.w.f.). The effects of hydrolysis temperature and alkali concentrations on wool properties were checked using optical and scanning electron microscopy. It was observed that the hydrolyzates obtained in both cases contained low molecular weight proteins and amino acids. Both the hydrolysis processes resulted in degradation of the wool fibers. However, superheated steam hydrolysis is an environmentally friendly and less expensive process, as it is performed using water as a solvent. The wool hydrolyzates produced using superheated water hydrolysis could find a potential application in agriculture, such as fertilization, soil improvement and suchlike.
Source: crossref · Quality: baseline
Research context
OpenAlex topics: Dyeing and Modifying Textile Fibers · Enzyme-mediated dye degradation · Silk-based biomaterials and applications
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
Affiliations
Italian National Research Council, Institute for Macromolecular Studies, Italy
Politecnico di Torino, DISAT – Department of Applied Science and Technology, Italy
References (30)
Show source-provided references
1. 10.1016/j.ijbiomac.2007.03.00210.1016/j.ijbiomac.2007.03.002 ↗
2. 10.1007/s12649-015-9393-010.1007/s12649-015-9393-0 ↗
3. 10.1016/j.wasman.2009.03.00910.1016/j.wasman.2009.03.009 ↗
4. 10.1016/j.resconrec.2014.01.00410.1016/j.resconrec.2014.01.004 ↗
5. 10.1016/0960-8524(94)90156-210.1016/0960-8524(94)90156-2 ↗
6. 10.1016/j.chemosphere.2008.03.06310.1016/j.chemosphere.2008.03.063 ↗
7. 10.2174/138945011131405001010.2174/1389450111314050010 ↗
8. 10.1016/j.molstruc.2010.01.04810.1016/j.molstruc.2010.01.048 ↗
9. 10.1016/j.biomaterials.2009.09.07610.1016/j.biomaterials.2009.09.076 ↗
10. 10.1016/j.biortech.2005.05.02110.1016/j.biortech.2005.05.021 ↗
11. 10.1007/s11274-005-9045-910.1007/s11274-005-9045-9 ↗
12. 10.1021/am508498u10.1021/am508498u ↗
13. 10.1039/c2gc36243k10.1039/c2gc36243k ↗
14. 10.1021/bm060597w10.1021/bm060597w ↗
15. 10.1021/bm060811g10.1021/bm060811g ↗
16. 10.1137/011103010.1137/0111030 ↗
17. 10.1038/227680a010.1038/227680a0 ↗
18. 10.1177/00405175810510020910.1177/004051758105100209 ↗
19. Choudhury AKR · 2006
20. Zhang H · Ind Textila · 2014 · 65 · 123
21. 10.1177/00405175670370100410.1177/004051756703701004 ↗
22. 10.1007/978-94-011-0595-810.1007/978-94-011-0595-8 ↗
23. 10.1016/j.tibtech.2004.02.00810.1016/j.tibtech.2004.02.008 ↗
24. 10.1177/00405175360060060510.1177/004051753600600605 ↗
25. Horio M, Kondo T and Sekimoto K. Pyrolysis of wool in sealed tubes. In: Proceedings of the International Wool Textile Research conference, Paris, 1965, vol. 2, p. 189. France: Institut Textile de France.
26. Lewin M · 2007
27. 10.1080/1944702640866242510.1080/19447026408662425 ↗
28. 10.1201/978143982346010.1201/9781439823460 ↗
29. 10.1016/j.molstruc.2009.08.03610.1016/j.molstruc.2009.08.036 ↗
30. 10.1002/app.3653510.1002/app.36535 ↗