Source abstract
Abstract
Abstract We study the mitigation of light- and elevated temperature-induced degradation (LeTID) with high-intensity illumination treatments, placing special emphasis on inline feasibility. After the treatments, we investigate the stability upon degradation conditions close to the recently suggested standard, which allows estimating the LeTID behavior during the operating lifetime of solar modules in the field. Subsequently, we map the stability at different treatment intensities and temperatures achievable with an air-cooled tool. We show that, when applying short treatment times, the stability improves with increasing treatment intensity and deteriorates steeply with rising temperature above an optimum region around 250 °C. However, these intensity- and temperature-dependent differences largely vanish when increasing the treatment time sufficiently. We also investigate the significance of darkness/illumination during the cooling ramp from the treatment temperature in view of the LeTID stability. We discuss our results based on suggested defect models of LeTID, and provide hypotheses of the origin of the instabilities observed at the high treatment temperatures. After identifying optimal treatments, we demonstrate that the energy yield loss due to LeTID reduces by over 60% after an inline-feasible process consisting of only 30 s of high-intensity illumination, combined with cooling of the samples from the process temperature under a lower-intensity illumination.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Silicon and Solar Cell Technologies · Thin-Film Transistor Technologies · Photovoltaic System Optimization Techniques
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (45)
Show source-provided references
1. Fundamental boron-oxygen-related carrier lifetime limit in mono- and multicrystalline silicon10.1002/pip.586 ↗
2. Degradation of multicrystalline silicon solar cells and modules after illumination at elevated temperature10.1016/j.solmat.2015.06.015 ↗
3. Ramspeck · 2012 · 861
4. Light-induced degradation of PECVD aluminium oxide passivated silicon solar cells10.1002/pssr.201409424 ↗
5. Brand · 2017 · 382
6. Mass production of p-type Cz silicon solar cells approaching average stable conversion efficiencies of 22 %10.1016/j.egypro.2017.09.308 ↗
7. Dependence of LeTID on brick height for different wafer suppliers with several resistivities and dopants
8. Light-induced degradation in quasi-monocrystalline silicon PERC solar cells: indications on involvement of copper
9. Hydrogen induced degradation: a possible mechanism for light- and elevated temperature-induced degradation in n-type silicon10.1016/j.solmat.2018.05.034 ↗
10. Temperature dependent degradation and regeneration of differently doped mc-Si materials10.1016/j.egypro.2017.09.085 ↗
11. Lifetime degradation in multicrystalline silicon under illumination at elevated temperature: indications for the involvement of hydrogen10.1063/1.5049320 ↗
12. Carrier-induced degradation in multicrystalline silicon: dependence on the silicon nitride passivation layer and hydrogen released during firing10.1109/JPHOTOV.2017.2783851 ↗
13. Understanding the light-induced degradation at elevated temperatures: similarities between multicrystalline and floatzone p-type silicon10.1002/pip.2954 ↗
14. Influence of temperature on light induced phenomena in multicrystalline silicon10.1063/1.5049326 ↗
15. Influence of bound hydrogen states on carrier-induced degradation in multi-crystalline silicon10.1063/1.5049323 ↗
16. On the defect physics behind light and elevated temperature-induced degradation (LeTID) of multicrystalline silicon solar cells10.1109/JPHOTOV.2019.2937223 ↗
17. Engineering solutions and root-cause analysis for light-induced degradation in p-type multicrystalline silicon PERC modules10.1109/JPHOTOV.2016.2556981 ↗
18. Intra-grain versus grain boundary degradation due to illumination and annealing behavior of multi-crystalline solar cells10.1016/j.solmat.2016.05.061 ↗
19. Recovery of LeTID by low intensity illumination: reaction kinetics, completeness and threshold temperature10.1016/j.egypro.2017.09.090 ↗
20. A four-state kinetic model for the carrier-induced degradation in multicrystalline silicon: introducing the reservoir state10.1016/j.solmat.2018.04.024 ↗
21. The role of dark annealing in light and elevated temperature induced degradation in p-type mono-like silicon10.1109/JPHOTOV.2020.2993653 ↗
22. Low-temperature dark anneal as pre-treatment for LeTID in multicrystalline silicon10.1016/j.solmat.2018.12.021 ↗
23. Optimization of belt furnace anneal to reduce light and elevated temperature induced degradation of effective carrier lifetime of P-type multicrystalline silicon wafers10.1002/solr.201800070 ↗
24. Firing temperature profile impact on light induced degradation in multicrystalline silicon10.1016/j.egypro.2017.09.082 ↗
25. Rapid stabilization of high-performance multicrystalline P-type silicon PERC cells10.1109/JPHOTOV.2016.2606704 ↗
26. Assessing the impact of thermal profiles on the elimination of light- and elevated-temperature-induced degradation10.1109/JPHOTOV.2018.2874769 ↗
27. Eliminating light- and elevated temperature-induced degradation in P-type PERC solar cells by a two-step thermal process10.1016/j.solmat.2020.110470 ↗
28. Annealing prior to contact firing: a potential new approach to suppress LeTID10.1016/j.solmat.2019.109938 ↗
29. Rapid passivation of carrier-induced defects in p-type multi-crystalline silicon10.1016/j.solmat.2016.05.022 ↗
30. Acceleration and mitigation of carrier-induced degradation in p-type multi-crystalline silicon10.1002/pssr.201510437 ↗
31. Fast regeneration processes to avoid light-induced degradation in multicrystalline silicon solar cells10.1109/JPHOTOV.2016.2598273 ↗
32. Instability of increased contact resistance in silicon solar cells following post-firing thermal processes10.1002/solr.201700129 ↗
33. Modulation of carrier-induced defect kinetics in multi-crystalline silicon PERC cells through dark annealing10.1002/solr.201600028 ↗
34. Impact of dark annealing on the kinetics of light- and elevated-temperature-induced degradation10.1109/JPHOTOV.2018.2866325 ↗
35. Herguth · 2019 · 116
36. Iron-boron pairing kinetics in illuminated p-type and in boron/phosphorus co-doped n-type silicon10.1063/1.4889817 ↗
37. Carrier-diffusion corrected J0-analysis of charge carrier lifetime measurements for increased consistency10.1016/j.solmat.2015.06.043 ↗
38. Wilking · 2014 · 366
39. Degradation of surface passivation on crystalline silicon and its impact on light-induced degradation experiments10.1109/JPHOTOV.2017.2755072 ↗
40. Bulk and surface-related degradation in lifetime samples made of czochralski silicon passivated by plasma-enhanced chemical vapor deposited layer stacks10.1002/pssa.201800741 ↗
41. On effective surface recombination parameters10.1063/1.4886595 ↗
42. On the lifetime-equivalent defect density: properties, application, and pitfalls10.1109/JPHOTOV.2019.2922470 ↗
43. Vahlman · 2020 · 409
44. Investigation of temperature and illumination dependencies of carrier-induced degradation in p-type multi-crystalline silicon10.1063/1.5049333 ↗
45. OriginPro 9.1: scientific data analysis and graphing software-software review10.1021/ci500161d ↗