Wide-optical bandgap with improved conductivity p-μc-Si:Ox:H films prepared by Cat-CVD
Source abstract
Abstract
Abstract Boron-doped hydrogenated microcrystalline silicon oxide ( p-μc- Si:O x :H) films have been deposited using catalytic chemical vapor deposition (Cat-CVD). The single-coiled tungsten catalyst temperature ( T fil ) was varied from 1850 to 2100 °C and films were deposited on glass substrates at the temperatures ( T sub ) of 100–300 °C. Different catalyst-to-substrate distances of 3–5 cm and deposition pressures from 0.1 to 0.6 Torr were considered. Optical and electrical characterizations have been made for the deposited samples. The sample transmittance measurement shows an optical-bandgap (Eg opt ) variation from 1.74 to 2.10 eV as a function of the catalyst and substrate temperatures. One of the best window materials was obtained at T sub =100 °C and T fil =2050 °C, with Eg opt =2.10 eV, dark conductivity of 3.0×10 −3 S cm −1 and 0.3 nm s −1 deposition rate.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Thin-Film Transistor Technologies · Silicon Nanostructures and Photoluminescence · Phase-change materials and chalcogenides
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References
Reference metadata was not supplied for this record.