High rate deposition and in situ doping of silicon films for solar cells on glass
Source abstract
Abstract
Abstract For solar cells on low cost float glass substrates a thickness of 20 μm of a poly-Si film is sufficient to absorb light. Between the substrate and active layer a combination of metal nitride and graphite enables the recrystallization of the nanocrystalline deposited silicon. Efficient deposition rates for the in situ p-doped Si absorber up to 300 nm/min are achieved by means of a PECVD process in combination with trichlorosilane (SiHCl 3 ), boron trichloride (BCl 3 ) and hydrogen (H 2 ). The substrate temperature is chosen between 770 and 820 K. The active Si films are recrystallized by a line-shaped electron beam which crosses the substrate at velocity up to 10 cm/s.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Thin-Film Transistor Technologies · Silicon Nanostructures and Photoluminescence · Silicon and Solar Cell Technologies
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (7)
Show source-provided references
1. High rate deposition and electron beam recrystallization of silicon films for solar cells10.1016/S0040-6090(01)01617-0 ↗
2. Low temperature growth of silicon-boron layer by ultrahigh vacuum chemical vapour deposition10.1063/1.111777 ↗
3. Eustathopoulos · 1999
4. The deposition mechanism of diamond-like a-C and a-C:H10.1016/0925-9635(94)90186-4 ↗
5. T. Kieliba, S. Reber, Enhanced zone-melting recrystallization for crystalline silicon thin-film solar cells, Proceedings of 16th European PVSEC 2000, Glasgow, United Kingdom.
6. A line beam electron gun for rapid thermal processing10.1063/1.1143152 ↗
7. Hebling · 1999