Dominant parameter determining dangling-bond density in hydrogenated amorphous silicon films prepared by catalytic chemical vapor deposition

Atsushi Masuda, Chisato Niikura, Yoriko Ishibashi, Hideki Matsumura

Publisher page

Abstract

Abstract It is found that one of the dominant parameters in determining the dangling-bond (DB) density in hydrogenated amorphous silicon (a-Si:H) films prepared by catalytic chemical vapor deposition (Cat-CVD), often called hot-wire CVD, is the catalyzer-surface area. a-Si:H films with an initial DB density of 4×1015 cm−3 and a saturated one after light soaking of 3×1016 cm−3 are prepared by Cat-CVD with a deposition rate of 11 A/s. “Catalytic plate” instead of the conventional wire is also proposed in order to suppress the heat radiation from the catalyzer while keeping the catalyzer surface area constant.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Thin-Film Transistor Technologies · Silicon Nanostructures and Photoluminescence · Transition Metal Oxide Nanomaterials

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (5)

Show source-provided references
1. Matsumura · J. Appl. Phys. · 1989 · 65 · 439610.1063/1.343278 ↗
2. Mahan · J. Appl. Phys. · 1991 · 69 · 672810.1063/1.348897 ↗
3. Niikura · J. Appl. Phys. · 1999 · 86 · 98510.1063/1.370836 ↗
4. Langford · Phys. Rev. B · 1992 · 45 · 1336710.1103/PhysRevB.45.13367 ↗
5. T. Takagi, R. Hayashi, A. Payne, W. Futako, T. Nishimoto, M. Takai, M. Kondo, A. Matsuda, High-rate growth of stable a-Si:H, Mater. Res. Soc. Symp. Proc. 557 (1999) 105.10.1557/PROC-557-105 ↗