Quality evaluation and improvement of iron-doped electromagnetic multycrystalline silicon wafers
Source abstract
Abstract
The effect of iron doping in electromagnetic cast (EMC) Si wafers on minority carrier recombination lifetime has been extensively investigated by means of microwave detected photo-conductivity decay (μ-PCD) and surface photo-voltage (SPV) to discriminate impurities and defects for the lower crystal quality. Optical and thermal activations of doped iron are investigated to study the difference between the two techniques in obtaining iron concentration. Minority carrier lifetimes increase or decrease after activation due to the different optical injection levels of both the SPV and μ-PCD techniques. No noticeable effect of chemical passivation in obtained iron concentration is observed. Boron and phosphorus gettering and hydrogen passivation techniques are applied to improve minority carrier recombination lifetime. As a result, the crystal quality of the EMC Si wafers depends on defect centers rather than on iron impurities.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Silicon and Solar Cell Technologies · Semiconductor materials and interfaces · Integrated Circuits and Semiconductor Failure Analysis
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (20)
Show source-provided references
1. K. Kaneko, R. Kawamura, H. Mizumoto,T. Misawa, Proceedings of the 11th E.C. PVSEC, Montreux, 1992, pp. 1070–1073.
2. K. Kaneko, T. Misawa, Technical Digest of the International PVSEC-7, Nagoya, Japan, 1993, p. 67.
3. Kittler · J. Appl. Phys. · 1995 · 77 · 372510.1063/1.358611 ↗
4. Zoth · J. Appl. Phys. · 1990 · 67 · 676410.1063/1.345063 ↗
5. Graff · Electrochem. Soc. · 1981 · 128 · 66910.1149/1.2127478 ↗
6. Wunstel · Appl. Phys. A · 1982 · 27 · 20710.1007/BF00619081 ↗
7. Weber · Appl. Phys. A · 1983 · 30 · 110.1007/BF00617708 ↗
8. K. Mishera, Electrochemical Society Proceedings 92:2, Extended Abstracts 426, October 1992, Toronto, Canada.
9. H. Hashizumme, S. Sumie, Y. Nakai, Recombination lifetime measurements in silicon, ASTM STP 1340, 1998.
10. Sopori · Mater. Sci. Fourm · 1997 · 258 · 52710.4028/www.scientific.net/MSF.258-263.527 ↗
11. Shockley · Phys. Rev. · 1952 · 87 · 83510.1103/PhysRev.87.835 ↗
12. Hall · IEE B · 1960 · 106 · 923
13. Lagowski · Appl. Phys. Lett. · 1993 · 63 · 304310.1063/1.110789 ↗
14. Kimmerling · Physica B · 1983 · 116 · 29710.1016/0378-4363(83)90263-2 ↗
15. Wijaranakula · J. Electrochem. Soc. · 1993 · 140 · 27510.1149/1.2056102 ↗
16. D.K. Schroder, Semiconductor and Material Device Characterization, Wiley-Interscince, New York, 1990. p. 435.
17. Buczkowski · J. Electrochem. Soc. · 1993 · 140 · 324010.1149/1.2221017 ↗
18. Lemke · Phys. Stat. Sol. A · 1981 · 64 · 21510.1002/pssa.2210640123 ↗
19. Bailey · Phys. Stat. Sol A · 1993 · 137 · 51510.1002/pssa.2211370221 ↗
20. Weber · 1998 · 18