Abstract

Abstract Material property differences are observed in hydrogenated microcrystalline silicon (μc-Si:H) thin films deposited under the same nominal conditions in a single-chamber plasma enhanced chemical vapor deposition system but at different stages of chamber history during prolonged usage. This phenomenon is called system shift, which results from the increase of powder coverage on the surface of the cathode and the coatings on other areas in the chamber. We propose a pre-hydrogen glow method to suppress the system shifting. Experimental results show that this method is very effective to reduce the non-reproducibility in μc-Si:H depositions for prolonged usage of the deposition system. In addition, the μc-Si:H films deposited with the pre-hydrogen glow have an improved structural homogeneity along the film thickness.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Thin-Film Transistor Technologies · Silicon Nanostructures and Photoluminescence

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (16)

Show source-provided references
1. Device grade microcrystalline silicon owing to reduced oxygen contamination10.1063/1.117440 ↗
2. Intrinsic microcrystalline silicon: a new material for photovoltaics10.1016/S0927-0248(99)00140-3 ↗
3. Recent progress in micromorph solar cells10.1016/S0022-3093(98)00352-4 ↗
4. Fabrication of intrinsic microcrystalline silicon thin films used for solar cells and its structure10.7498/aps.54.4874 ↗
5. Single-chamber deposition of intrinsic microcrystalline silicon thin filma and its application in solar cells
6. Hydrogenated microcrystalline silicon: how to correlate layer properties and solar cell performance10.1016/S0022-3093(99)00910-2 ↗
7. Doped-chamber deposition of intrinsic microcrystalline silicon thin films and its application in solar cells
8. Influence of boron on the properties of intrinsic microcrystalline silicon thin films10.7498/aps.58.1293 ↗
9. C. Droz, E. Vallat-Sauvain, J. Bailat, L. Feitknecht, A. Shah, Application of Raman spectroscopy for the microstructure characterisation in microcrystalline silicon solar cells, in: Proceedings of the 17th European Photovoltaic Solar Energy Conference, Münich, Germany, 2001, pp. 2917–2920.
10. X.D. Zhang, F.H. Sun, G.H. Wang, S.Z. Xu, C.C. Wei, J. Sun, X.H. Geng, S.Z. Xiong, Y. Zhao, Study of reduced the p/i interface boron contamination in single PECVD chamber deposition microcrystalline silicon solar cells, in: Proceedings of the 23rd European Photovoltaic Solar Energy Conference, Valencia, Spain, 2008, pp. 2297–2300.
11. Performance optimization of p–i–n type microcrystalline silicon thin films solar cells deposited in single chamber10.7498/aps.59.1344 ↗
12. Combined effect of electrode gap and radio frequency on power deposition and film growth kinetics in SiH4/H2 discharges10.1116/1.1421599 ↗
13. Ion bombardment effects on microcrystalline silicon growth mechanisms and on the film properties10.1063/1.1524707 ↗
14. Growth mechanism of microcrystalline silicon obtained from reactive plasmas10.1016/S0040-6090(98)01165-1 ↗
15. Fabrication of high growth rate solar-cell-quality μc-Si:H thin films by VHF-PECVD10.1088/1009-1963/13/8/034 ↗
16. Research on the boron contamination at the p/i interface of microcrystalline silicon solar cells deposited in a single PECVD chamber10.1088/1674-1056/18/10/077 ↗