Deposition behaviour of metal impurities in acidic cleaning solutions and their impact on effective minority carrier lifetime in n-type silicon solar cells
Source abstract
Abstract
Abstract Further increasing the conversion efficiency of silicon solar cells by advanced solar cell concepts like SHJ (Silicon Hetero-Junction), PERT (Passivated Emitter Rear Totally diffused), IBC (Interdigitated Back-Contact), requires a highly controlled silicon surface in terms of metal impurity density. The goal of this study is investigating the deposition property of different metals in acidic cleaning solutions and consequently determining the impact of these impurities on the effective minority lifetime of the crystalline silicon solar cell material. The deposition behaviour of impurities is mathematically described with an adsorption isotherm theory. Once attached at the silicon surface, the metal impurity can diffuse into the silicon bulk material during a high temperature process step like diffusion, passivation or contact annealing (firing). First, we have studied the adsorption isotherm behaviour of prominent metal impurities (Fe, Cu, Ti, Co, Cr and Zn) in acidic liquid onto a silicon surface. Moreover, the impact of metal impurities on effective minority carrier lifetime in commercially available n-type Cz-silicon (3–5 Ω cm, 239 cm2) is determined. From controlled contamination experiments we can extract an exchange volume, that provides the minimum amount on wet chemical cleaning solution that is required to clean a silicon surface from a given high metal impurity level to a specified low metal impurity level. This exchange volume plays a crucial role by defining feed and bleed recipes on wet chemical cleaning tanks in solar cell manufacturing. A second parameter extracted is the effective minority carrier lifetime degradation of the metal impurities. After deposition on the surface, the impurities are driven into the silicon bulk by high temperature processes. Depending on the lifetime degradation capacity, a relation of effective minority carrier lifetime versus surface contamination level could be identified for each metal impurity. We found Co, Fe and Cu having a strong impact on effective minority carrier lifetime degradation, e.g. 2e10/cm2 Fe surface concentration can reduce the effective minority carrier lifetime by 75%, while Ti, Zn and Cr are more moderate and only high surface concentrations above 1e12/cm2 lead to effective minority carrier lifetime degradation of more than 20% compared to the non-contaminated wafers.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Silicon and Solar Cell Technologies · Integrated Circuits and Semiconductor Failure Analysis · Thin-Film Transistor Technologies
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (17)
Show source-provided references
1. Evolutionary process development towards next generation crystalline silicon solar cells: a semiconductor process toolbox application10.1051/epjpv/2012009 ↗
2. John · 2018
3. Impurities in silicon solar cells10.1109/T-ED.1980.19922 ↗
4. Reduced fill factors in multicrystalline silicon solar cells due to injection-level dependant bulk recombination lifetimes10.1002/1099-159X(200007/08)8:4<363::AID-PIP328>3.0.CO;2-Y ↗
5. Transition metals in silicon10.1007/BF00617708 ↗
6. Iron contamination in silicon technology, applied physics A, Jan 2000[5] A.A. Istratov, E.R.Weber, E.R.,Physics of copper in Silicon10.1149/1.1421348 ↗
7. Impact of metal contamination in silicon solar cells10.1002/adfm.201000849 ↗
8. Recombination activity of interstitial iron and other transition metal point defects in p-and n-type crystalline silicon10.1063/1.1812833 ↗
9. Impurity-related limitations of next-generation industrial silicon solar cells10.1109/JPHOTOV.2012.2210030 ↗
10. Nobel Lecture, December 14, 1932
11. Masel · 1996 · 3
12. Competitive Adsorption of Metal Ions onto Hydrophilic Silicon Surfaces from Aqueous Solution10.1149/1.1391670 ↗
13. ‘Just-clean-enough’: optimization of wet chemical cleaning processes for crystalline silicon solar cells10.4028/www.scientific.net/SSP.255.344 ↗
14. Validation of vapor phase decomposition–droplet collection–total reflection X-ray fluorescence spectrometry for metallic contamination analysis of silicon wafers10.1016/j.sab.2004.03.011 ↗
15. Contactless determination of current–voltage characteristics and minority‐carrier lifetimes in semiconductors from quasi‐steady‐state photoconductance data10.1063/1.117723 ↗
16. Photoluminescence imaging of silicon wafers10.1063/1.2234747 ↗
17. P.W. Mertens, M. Meuris, H.F. Schmidt, S. Verhaverbeke, M.M. Heyns, P. Carr, D. Gräf, A. Schnegg, M. Kubota, K. Dillenbeck, R. de Blank, Critical aspect of wafer cleaning and gate oxide integrity, in: Proceedings of the Satellite Symposium to ESSDERC, Grenoble, France, (The Electrochemical Society, Pennington, NJ), 87, 1993, pp. 93–15.