In-line measurement of “trench structures” caused by the texturization of mc-silicon solar cells
Source abstract
Abstract
Abstract Acidic texturing of multicrystalline silicon (mc-Si) wafers often leads to rough surfaces with strong etch attacks (trench structures), especially at sites with crystal defects. The appearance of trench structures on the wafer surface has been cited in earlier publications and has been often recognised as being harmful to solar cell performance [Mathijssen et al., 2009] . In this work, an in-line measurement method for these structures is presented, using a line camera system with diffuse illumination. The presented method can be used for the in-line quality control of the acidic texturization. The number of trench structures is quantified in the images via a newly developed algorithm by an adaptive threshold method. With the help of AFM images the measurement method could be regarded in detail. It has been shown that the true area fraction of trench structures only lies between 0.3% and 1.8% instead of 2–12%, which is estimated from measurements. As expected, the number of trench structures strongly depends on the texture strength and the number of crystal defects in as-cut material. Therefore, if the texturization method remains constant, it is possible to easily measure material quality by measuring the fraction of trench structures and the presented measurement method could be used as cheap alternative to photoluminescence measurements. The reliability of the algorithm is demonstrated by the correlation between material quality, texture strength and the resulting number of trench structures.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Silicon and Solar Cell Technologies · Thin-Film Transistor Technologies · Advanced Surface Polishing Techniques
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (11)
Show source-provided references
1. M. Zimmer, K. Birmann, J. Hilgert, J. Rentsch, NIR-spectroscopical process control for wet chemical processes, in: Proceedings of the 24th European Photovoltaic Solar Energy Conference, Hamburg, Germany, 2009, pp. 1101–1105.
2. H.W.D.L. Bätzner, A. Sauer, B. Hadam, L. Janßen, and T. Pletzer, Acidic wet chemical texturistion of mc-Si solar cells, in: Proceedings of the 22nd European Photovoltaic Solar Energy Conference, Milan, Italy, 2007, pp. 1715–1719.
3. S. Mathijssen, S. Braun, I. Melnyk, M. Michel, M. Schmidt, P. Fath, J. Prölß, S. Schotthöfer, O. Rogge, Survey of acid texturing and new innovative acid processes for mc solar wafers, in: Proceedings of the 24th European Photovoltaic Solar Energy Conference, Hamburg, Germany, 2009, pp. 1964–1967.
4. W. Kwapil, M. Kasemann, P. Gundel, M.C. Schubert, W. Warta, O. Breitenstein, J. Bauer, A. Lotnyk, J.-M. Wagner, P.C.P. Bronsveld, G. Coletti, Physical mechanisms of breakdown in multicrystalline silicon solar cells, in: Proceedings of the 24th European Photovoltaic Solar Energy Conference, Hamburg, Germany, 2009, pp. 896–900.
5. J. Haunschild, M. Glatthaar, W. Kwapil, S. Rein, Comparing luminescence imaging with illuminated lock-in thermography and carrier density imaging for inline inspection of silicon solar cells, in: Proceedings of the 24th European Photovoltaic Solar Energy Conference, Hamburg, Germany, 2009, pp. 857–862.
6. L. Korte, S. Bastide, C. Lévy-Clément, Fast measurements of effective optical reflectivity using a conventional flatbed scanner, in: Proceedings of the 23rd European Photovoltaic Solar Energy Conference, Valencia, Spain, 2008, pp. 1431–1437.
7. A. Krieg, J. Wallach, S. Rein, Impact of surface structures on the inline vision inspection of antireflection coatings, in: Proceedings of the 24th European Photovoltaic Solar Energy Conference, Hamburg, Germany, 2009, pp. 2041–2044.
8. M. Demant, M. Glatthaar, J. Haunschild, S. Rein, Analysis of luminescence images applying pattern recognition techniques, in: Proceedings of the 25th European Photovoltaic Solar Energy Conference and Exhibition, Valencia, Spain, 2010, pp. 1078–1082.
9. Quality control of as-cut multicrystalline silicon wafers using photoluminescence imaging for solar cell production10.1016/j.solmat.2010.06.003 ↗
10. A technique for delineating defects in silicon10.4028/www.scientific.net/SSP.82-84.753 ↗
11. An etch for delineation of defects in silicon10.1149/1.2115767 ↗