Microcrystalline and micromorph device improvements through combined plasma and material characterization techniques
Source abstract
Abstract
Hydrogenated microcrystalline silicon (µc-Si:H) growth by very high frequency plasma-enhanced chemical vapor deposition (VHF-PECVD) is studied in an industrial-type parallel plate KAI reactor. Combined plasma and material characterization techniques allow to assess critical deposition parameters for the fabrication of high quality material. A relation between low intrinsic stress of the deposited i-layer and better performing solar cell devices is identified. Significant solar cell device improvements were achieved based on these findings: high open circuit voltages above 520 mV and fill factors above 74% were obtained for 1 µm thick µc-Si:H single junction cells and a 1.2 cm2 micromorph device with 12.3% initial (Voc=1.33 V, FF=72.4%, Jsc=12.8 mA cm-2) and above 10.0% stabilized efficiencies.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Thin-Film Transistor Technologies · Silicon and Solar Cell Technologies · Silicon Nanostructures and Photoluminescence
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (13)
Show source-provided references
1. Plasma silane concentration as a determining factor for the transition from amorphous to microcrystalline silicon in SiH4/H2 discharges10.1088/0963-0252/16/1/011 ↗
2. Stress-induced nucleation of microcrystalline silicon from amorphous phase10.1143/JJAP.41.2821 ↗
3. The physics of plasma-enhanced chemical vapour deposition for large-area coating: industrial application to flat panel displays and solar cells10.1088/0741-3335/42/12B/326 ↗
4. Infrared laser-based monitoring of the silane dissociation during deposition of silicon thin films10.1063/1.3141520 ↗
5. Spectroscopic diagnostics and modelling of silane microwave plasmas10.1088/0741-3335/40/6/011 ↗
6. Fast equilibration of silane/hydrogen plasmas in large area RF capacitive reactors monitored by optical emission spectroscopy10.1088/0963-0252/16/4/001 ↗
7. Determination of Raman emission cross-section ratio in hydrogenated microcrystalline silicon10.1016/j.jnoncrysol.2005.11.128 ↗
8. Brenner · Calculation of stress in electrodeposits from the curvature of a plated strip, Journal of Research of the National Bureau of Standards · 1949 · 42 · 105
9. Calculated elastic constants for stress problems associated with semiconductor devices10.1063/1.1661935 ↗
10. J. Bailat, D. Domine, R. Schluchter, J. Steinhauser, S. Fay, F. Freitas, C. Bucher, L. Feitknecht, X. Niquille, T. Tscharner, A. Shah, C. Ballif, High-efficiency p-i-n microcrystalline and micromorph thin film silicon solar cells deposited on lpcvd zno coated glass substrates, in: Conference Record of the 2006 IEEE 4th World Conference on Photovoltaic Energy Conversion, vol. 2, 2006, pp. 1533–1536. URL: 〈http://dx.doi.org/10.1109/WCPEC.2006.279775〉 doi:10.1109/WCPEC.2006.279775.10.1109/WCPEC.2006.279775 ↗
11. High-rate deposition of microcrystalline silicon p-i-n solar cells in the high pressure depletion regime10.1063/1.2961334 ↗
12. Hydrogen in amorphous and microcrystalline silicon films prepared by hydrogen dilution10.1063/1.363541 ↗
13. Influence of pressure and silane depletion on microcrystalline silicon material quality and solar cell performance10.1063/1.3095488 ↗