Abstract

Abstract In the majority of studies involving injection dependent lifetime spectroscopy, it is assumed that the investigated defect is a single-level defect following Shockley-Read-Hall recombination statistics. Nevertheless, in real life, two-level defects or multi-level defects are more common than single-level defects. In this study, we first investigated the possible consequences of misinterpreting a two-level defect as two single-level defects. A procedure to properly fit two-level defects in lifetime spectroscopy is subsequently proposed. At the end, we use boron-oxygen related defects as an experimental demonstration. Our experimental results reveal that the recombination statistics of boron-oxygen related defects cannot be explained by the coexistence of two independent single-level defects. A two-level defect parameterization appears to be more suitable.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Electrochemical Analysis and Applications · Ion-surface interactions and analysis · Integrated Circuits and Semiconductor Failure Analysis

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (69)

Show source-provided references
1. Green · 1995
2. Graff · 2013
3. Rein · 2006
4. Temperature- and injection-dependent lifetime spectroscopy for the characterization of defect centers in semiconductors10.1063/1.1563830 ↗
5. Recombination parameters of lifetime-limiting carrier-induced defects in multicrystalline silicon for solar cells10.1063/1.4977906 ↗
6. New insights into the thermally activated defects in n-type float-zone silicon10.1063/1.5123901 ↗
7. Lifetime spectroscopy for defect characterization: systematic analysis of the possibilities and restrictions10.1063/1.1428095 ↗
8. Defect parameters contour mapping: a Powerful tool for lifetime spectroscopy data analysis10.1002/pssb.201800082 ↗
9. Application of the Newton–Raphson method to lifetime spectroscopy for extraction of defect parameters10.1109/JPHOTOV.2017.2695666 ↗
10. Reassessment of the recombination parameters of chromium in n- and p-type crystalline silicon and chromium-boron pairs in p-type crystalline silicon10.1063/1.4881497 ↗
11. Assessing the defect responsible for LeTID: temperature- and injection-dependent lifetime spectroscopy
12. Statistics of the recombination of holes and electrons10.1103/PhysRev.87.835 ↗
13. Electron-hole recombination in germanium10.1103/PhysRev.87.387 ↗
14. Electronic properties of light-induced recombination centers in boron-doped Czochralski silicon10.1063/1.371186 ↗
15. Electronic properties of the metastable defect in boron-doped Czochralski silicon: unambiguous determination by advanced lifetime spectroscopy10.1063/1.1544431 ↗
16. Electronically activated boron-oxygen-related recombination centers in crystalline silicon10.1063/1.2140584 ↗
17. Spatially resolved impurity identification via temperature-and injection-dependent photoluminescence imaging10.1109/JPHOTOV.2015.2447837 ↗
18. Synchrotron-based investigation of transition-metal getterability in n-type multicrystalline silicon10.1063/1.4950765 ↗
19. Advanced defect and impurity diagnostics in silicon based on carrier lifetime measurements10.1002/pssa.200564510 ↗
20. Determining the defect parameters of the deep aluminum-related defect center in silicon10.1063/1.2789378 ↗
21. Cobalt related defect levels in silicon analyzed by temperature- and injection-dependent lifetime spectroscopy10.1063/1.2433743 ↗
22. Electronic properties of titanium in boron-doped silicon analyzed by temperature-dependent photoluminescence and injection-dependent photoconductance lifetime spectroscopy10.1063/1.2996252 ↗
23. Lifetime-degrading boron-oxygen centres in p-type and n-type compensated silicon10.1063/1.3609069 ↗
24. Parameterisation of injection-dependent lifetime measurements in semiconductors in terms of Shockley-Read-Hall statistics: an application to oxide precipitates in silicon10.1063/1.4725475 ↗
25. Determining the charge states and capture mechanisms of defects in silicon through accurate recombination analyses: a review10.1016/j.solmat.2018.07.029 ↗
26. On the mechanism of recombination at oxide precipitates in silicon10.1063/1.4789858 ↗
27. Electrical characterization of the slow boron oxygen defect component in Czochralski silicon10.1002/pssr.201510357 ↗
28. Fast in-situ photoluminescence analysis for a recombination parameterization of the fast BO defect component in silicon10.1063/1.4961423 ↗
29. Recent insights into boron-oxygen related degradation: evidence of a single defect10.1016/j.solmat.2017.06.038 ↗
30. Injection dependent lifetime spectroscopy for two-level defects in silicon
31. Accurate defect recombination parameters: what are the limitations of current analyses?
32. Electron-hole recombination statistics in semiconductors through flaws with many charge conditions10.1103/PhysRev.109.1103 ↗
33. Lifetime spectroscopy investigation of light-induced degradation in p-type multicrystalline silicon PERC10.1109/JPHOTOV.2016.2606699 ↗
34. Investigation of photon and thermal induced change in silicon solar cells
35. Structure and transformation of the metastable boron- and oxygen-related defect center in crystalline silicon10.1103/PhysRevB.69.024107 ↗
36. Degradation of crystalline silicon due to boron–oxygen defects10.1109/JPHOTOV.2016.2614119 ↗
37. Kinetics of the electronically stimulated formation of a boron-oxygen complex in crystalline silicon10.1103/PhysRevB.76.035210 ↗
38. Analysis of the defect activation in CZ-silicon by temperature-dependent bias-induced degradation of solar cells, 3rd World
39. Investigation of carrier lifetime instabilities in Cz-grown silicon
40. Kinetics of the boron-oxygen related defect in theory and experiment10.1063/1.3517155 ↗
41. Deactivation of the boron-oxygen recombination center in silicon by illumination at elevated temperature10.1002/pssr.200802009 ↗
42. On the degradation of Cz-silicon solar cells, 2nd World
43. Comparison of boron- and gallium-doped p-type Czochralski silicon for photovoltaic application10.1002/(SICI)1099-159X(199911/12)7:6<463::AID-PIP293>3.0.CO;2-H ↗
44. Boron-oxygen defect imaging in p-type Czochralski silicon10.1063/1.4819096 ↗
45. Characterization of the initial rapid decay on light-induced carrier lifetime and cell performance degradation of Czochralski-grown silicon10.1143/JJAP.42.2564 ↗
46. Influence of net doping, excess carrier density and annealing on the boron oxygen related defect density in compensated n-type silicon10.1063/1.3633492 ↗
47. Fast and slow lifetime degradation in boron-doped Czochralski silicon described by a single defect10.1002/pssr.201600096 ↗
48. Modulating the extent of fast and slow boron-oxygen related degradation in Czochralski silicon by thermal annealing: evidence of a single defect10.1063/1.4975685 ↗
49. Impact of interstitial iron on the study of meta-stable B-O defects in Czochralski silicon: further evidence of a single defect10.1063/1.5000323 ↗
50. Fast and slow stages of lifetime degradation by boron‐oxygen centres in crystalline silicon
51. Identification of the mechanism responsible for the boron oxygen light induced degradation in silicon photovoltaic cells10.1063/1.5091759 ↗
52. Boron–oxygen complex responsible for light‐induced degradation in silicon photovoltaic cells: a new insight into the problem10.1002/pssa.201900315 ↗
53. The first 70 semiconductor Auger processes10.1016/0038-1101(78)90195-8 ↗
54. Trap‐Auger recombination in silicon of low carrier densities10.1063/1.98086 ↗
55. Light-induced-degradation defect independent of the boron concentration: towards unifying admittance spectroscopy, photoluminescence and photoconductance lifetime spectroscopy results10.1016/j.solmat.2020.110481 ↗
56. Astm-F1188
57. Permanent annihilation of thermally activated defects which limit the lifetime of float-zone silicon10.1002/pssa.201600360 ↗
58. Thermal activation and deactivation of grown-in defects limiting the lifetime of float-zone silicon10.1002/pssr.201600080 ↗
59. Quasi-steady-state photoconductance, a new method for solar cell material and device characterization
60. Photoluminescence: a surprisingly sensitive lifetime technique
61. Self-consistent calibration of photoluminescence and photoconductance lifetime measurements10.1063/1.2119411 ↗
62. Trapping and junction-related perturbations of the effective excess carrier lifetime, 3rd World
63. Oxygen-related minority-carrier trapping centers in p-type Czochralski silicon10.1063/1.1483908 ↗
64. Trapping of minority carriers in multicrystalline silicon10.1063/1.123663 ↗
65. On the use of a bias-light correction for trapping effects in photoconductance-based lifetime measurements of silicon10.1063/1.1346652 ↗
66. Reassessments of minority carrier traps in silicon with photoconductance decay measurements10.1109/JPHOTOV.2019.2903584 ↗
67. Overview on SiN surface passivation of crystalline silicon solar cells10.1016/S0927-0248(00)00099-4 ↗
68. Generalized procedure to determine the dependence of steady-state photoconductance lifetime on the occupation of multiple defects10.1063/1.2999640 ↗
69. Trapping artifacts in quasi-steady-state photoluminescence and photoconductance lifetime measurements on silicon wafers10.1063/1.2165274 ↗