N2O plasma treatment for minimization of background plating in silicon solar cells with Ni–Cu front side metallization
Source abstract
Abstract
In this paper we demonstrate that an additional nitrous oxide (N2O) plasma treatment step after the regular SiNx:H anti-reflective coating (ARC) deposition practically eliminates background plating during Ni–Cu contact metallization for c-Si solar cells. This step is relatively simple and could henceforth enable the commercialization of plated Ni–Cu contacts, which is currently inhibited by the creation of localized metal-silicon interfaces due to background plating, among other issues like adhesion. The average active area efficiency and fill-factor of reference cells without any plasma treatment are 17.4% and 73.5%, respectively. N2O plasma treatment before ARC deposition leads to an improved average fill-factor of 75.0%. This improvement is attributed to a reduction in the area affected by background plating by approximately 40% due to the formation of a thin silicon oxy-nitride layer. N2O plasma treatment after ARC deposition is even more effective and can overcome background plating with an average active area cell efficiency and fill-factor of 18.5% and 77.5%, respectively. This performance improvement is attributed to oxidation of the ARC surface by the plasma post-treatment. Analysis of background plating losses is complemented by current–voltage curve fits to a 3-diode model with resistance limited recombination, performed by the freely available program “2/3-Diode Fit”.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Silicon and Solar Cell Technologies · Thin-Film Transistor Technologies · Semiconductor materials and interfaces
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (32)
Show source-provided references
1. Ag requirements for silicon wafer-based solar cells10.1002/pip.1125 ↗
2. Economic evaluation of two-step metallization processes for silicon solar cells10.1016/j.egypro.2011.06.182 ↗
3. P. Verlinden, Cost analysis of current PV production and strategy for future silicon PV modules, in: Proceedings of the 28th European Photovoltaic Conference and Exhibition, Paris, September 2013.
4. Review of Ni–Cu based front side metallization for c-Si solar cells10.1155/2013/183812 ↗
5. Evolution of metal plating for silicon solar cell metallisation10.1002/pip.2221 ↗
6. International Technology Roadmap for Photovoltaics (ITRPV) Results 2013, fifth edition, March, 2014.
7. Experimental study on the elimination of over-plating problems in industrial manufacturing of large-area acidic-textured laser-doped multi-crystalline solar cells10.1016/j.solmat.2012.08.019 ↗
8. The origin of background plating10.1016/j.egypro.2011.06.183 ↗
9. Overcoming over-plating problems for PECVD SiNx passivated laser doped p-type multi-crystalline silicon solar cells10.1016/j.solmat.2011.12.003 ↗
10. B. Tjahjono, S. Wang, A. Sugianto, L. Mai, Z. Hameiri, N. Borojevic, A. Ho-Baillie, S. Wenham, Application of laser doped contact structure on multicrystalline solar cells, in: Proceedings of the 23rd EU PVSEC, Valencia, September 2008, pp. 195–2000.
11. Improved LDSE processing for the avoidance of overplating yielding 19.2% efficiency on commercial grade crystalline Si solar cell10.1016/j.solmat.2011.07.030 ↗
12. Stanley Wang, T. Puzzer, B. Vogl, B. Tjahjono, B. Hallam, M. Eadie, N. Borojevic, Z. Hameiri, S. Wenham, Overcoming over-plating problems on acid textured multicrystalline wafers with silicon nitride coated surfaces, in: Proceedings of 24th EUPVSEC, Hamburg, September 2009, pp. 1449–1452.
13. SiOx(C)/SiNx dual-layer anti-reflectance film coating for improved cell efficiency10.1016/j.solener.2011.09.007 ↗
14. Mehul C. Raval, Stephan Suckow, Chetan Singh Solanki, Analysis of background plating for Ni–Cu based metallization by observing local ideality factor variation, in: Proceedings of the 29th EU PVSEC, Amsterdam, September 2014.
15. James A. Gregory, Method of Fabricating Solar Cell, US Patent No. 4,650,695, 1987.
16. Gary Hamm, David L. Jacques, Carl J. Colangelo, Method of Inhibiting Background Plating, U.S. Patent No. 7,939,438 B2, 2011.
17. McIntosh · 2001
18. Stephan Suckow, 2/3-Diode Fit. 〈http://nanohub.org/resources/14300〉, 2014.
19. Chaudhari · 2010
20. Electrodeposition of tin: a simple approach
21. ImageJ software Link-〈http://imagej.nih.gov/ij/〉
22. A.G. Aberle, S.R. Wenham, M.A. Green, A new method for accurate measurements of the lumped series resistance of solar cells, in: Proceedings of the 23rd IEEE Photovoltaic Specialists Conference, Louisville, 1993, pp. 133–139.10.1109/PVSC.1993.347065 ↗
23. Dicker · 2003
24. R.A. Sinton, A. Cuevas, A quasi-steady state open-circuit voltage method for solar cell characterization, in: Proceedings of 16th EUPVSEC, Glasgow, 2000, pp. 1152–1155.
25. F. Hernando, R. Gutierrez, G. Bueno, F. Recart, V. Rodriguez, Humps, a surface damage explanation, in: Proceedings of 15th EC PVSEC, Vienna, 1998, pp. 1321–1323.
26. Plasma grown oxy-nitride films for silicon surface passivation10.1109/LED.2013.2263331 ↗
27. Visible photoluminescence from silicon nanoclusters embedded in silicon nitride films prepared by remote plasma-enhanced chemical vapor deposition10.1016/j.physe.2006.12.047 ↗
28. Accuracy of analytical expressions for solar cell fill factors10.1016/0379-6787(82)90057-6 ↗
29. Bonding structure of silicon oxynitride grown by plasma-enhanced chemical vapor deposition10.1143/JJAP.46.3202 ↗
30. XPS and FTIR study of silicon oxynitride thin films10.1016/S0955-2219(97)00051-4 ↗
31. Surface oxidation of silicon nitride films10.1149/1.2132877 ↗
32. Plasma treatment of porous SiNx:H films for the fabrication of porous-dense multilayer optical filters with tailored interfaces10.1063/1.2202692 ↗