Photobleaching of MEH-PPV thin films: Correlation between optical properties and the nanoscale surface photovoltage
Source abstract
Abstract
Abstract The electro-optical properties of Poly[2-methoxy-5-(2-ethylhexyloxy)-1,4-phenylenevinylene] (MEH-PPV) thin films have been studied while the sample is illuminated with blue light. By combining Kelvin probe microscopy with classical optical techniques it has been possible to monitor the evolution of the nanoscale contact potential, the surface photovoltage and the optical properties of the material establishing a correlation between them. Contrary to what is usually accepted, it has been found that the nanoscale surface photovoltage is larger when the polymer is already photobleached. In addition, it has been possible to distinguish between the photophysical processes that govern the working principle of a polymer-based device and the photochemical reactions that degrade the material. Although complex charges trapping phenomena take place during the irradiation, the surface photovoltage effect depends only on the number of photons that have reached the polymer.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Organic Electronics and Photovoltaics · Force Microscopy Techniques and Applications · Conducting polymers and applications
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (45)
Show source-provided references
1. Conjugated polymer-based organic solar cells10.1021/cr050149z ↗
2. Photoactive nanostructures of polypyrrole10.1002/cphc.200800773 ↗
3. Molecular photovoltaics in nanoscale dimension10.3390/ijms12010173 ↗
4. Excited state and charge photogeneration dynamics in conjugated polymers10.1021/jp068864f ↗
5. Controlling interchain interactions in conjugated polymers: the effects of chain morphology on exciton–exciton annihilation and aggregation in MEH-PPV films10.1021/jp993190c ↗
6. Conjugated polymers as molecular materials: how chain conformation and film morphology influence energy transfer and interchain interactions10.1146/annurev.physchem.54.011002.103811 ↗
7. Excited state dynamics of a conformationally disordered conjugated polymer:a comparison of solutions and film10.1016/j.chemphys.2005.04.001 ↗
8. Polymeric thin films for organic electronics: properties and adaptive structures10.3390/ma6031159 ↗
9. Studies of the interface of conducting polymers with inorganic surfaces10.1007/s00216-012-6455-z ↗
10. Stability/degradation of polymer solar cells10.1016/j.solmat.2008.01.005 ↗
11. Surface photovoltage phenomena: theory, experiment, and applications10.1016/S0167-5729(99)00002-3 ↗
12. Photoinduced charge carriers at surfaces and interfaces of poly[2-methoxy-5-(2'-ethyl-hexyloxy)-1,4-phenylene vinylene] with Au and GaAs10.1103/PhysRevB.64.035325 ↗
13. Construction of the energy diagram of an organic semiconductor film on SnO2: F by surface photovoltage spectroscopy10.1016/S0925-3467(97)00086-4 ↗
14. Kelvin probe force microscopy10.1063/1.105227 ↗
15. Kelvin probe force microscopy study on conjugated polymer/fullerene bulk heterojunction organic solar cells10.1021/nl048176c ↗
16. Efficiency limiting morphological factors of MDMO-PPV: PCBM plastic solar cells10.1016/j.tsf.2005.12.071 ↗
17. Time-resolved opto-electronic properties of poly(3-hexylthiophene-2,5-diyl) fullerene heterostructures detected by Kelvin force microscopy10.1016/j.tsf.2010.08.132 ↗
18. Correlation between surface photovoltage and blend morphology in polyfluorene-based photodiodes10.1021/nl047929s ↗
19. Heterogeneity in polymer solar cells: local morphology and performance in organic photovoltaics studied with scanning probe microscopy10.1021/ar900231q ↗
20. Imaging the carrier photogeneration in nanoscale phase segregated organic heterojunctions by Kelvin probe force microscopy10.1021/nl101001d ↗
21. Nanoscale quantitative measurement of the potential of charged nanostructures by electrostatic and Kelvin probe force microscopy: unraveling electronic processes in complex materials10.1021/ar900247p ↗
22. Scanning Kelvin probe microscopy on bulk heterojunction polymer blends10.1002/adfm.200801283 ↗
23. Nanoscale surface photovoltage of organic semiconductors with two pass Kelvin probe microscopy10.1088/0957-4484/22/37/375704 ↗
24. 1997 · 3
25. Nanoscale electro-optical properties of organic semiconducting thin films: from individual materials to the blend10.1021/jp304278w ↗
26. Light-induced degradation of the active layer of polymer-based solar cells10.1016/j.polymdegradstab.2009.11.021 ↗
27. Measurement of the photobleaching kinetics of semiconducting polymer films by the pump-probe method10.1070/QE2011v041n12ABEH014715 ↗
28. Photogeneration and ultrafast dynamics of excitons and charges in P3HT/PCBM blends10.1021/jp807249b ↗
29. Electronic energy transfer and quantum-coherence in pi-conjugated polymers10.1021/cm102360x ↗
30. Enhancing dynamic scanning force microscopy in air: as close as possible10.1088/0957-4484/20/8/085707 ↗
31. WSXM: a software for scanning probe microscopy and a tool for nanotechnology10.1063/1.2432410 ↗
32. Wavelength dependence of nanoscale photodegradation in poly(3-octylthiophene) thin films10.1016/j.polymdegradstab.2011.04.002 ↗
33. Demonstration of absorbance using digital color image analysis and colored solutions10.1021/ed083p644 ↗
34. In-situ monitoring of surface chemistry and charge transfer at semiconductor surfaces10.1016/S0169-4332(96)00121-3 ↗
35. Optical constants of conjugated polymer/fullerene based bulk-heterojunction organic solar cells10.1080/713738799 ↗
36. On the photochemical stability of dialkoxy-PPV; a quantitative approach10.1098/rsta.1997.0036 ↗
37. In situ characterization of the oxidative degradation of a polymeric light emitting device10.1063/1.365493 ↗
38. Singlet oxygen as a reactive intermediate in the photodegradation of phenylenevinylene oligomers10.1021/cm9807687 ↗
39. Singlet oxygen as a reactive intermediate in the photodegradation of an electroluminescent polymer10.1021/ja00146a004 ↗
40. Durability of MDMO-PPV and MDMO-PPV: PCBM blends under illumination in the absence of oxygen10.1016/j.solmat.2007.12.003 ↗
41. Photo-oxidation in an O-18(2) atmosphere: a powerful tool to elucidate the mechanism of UV–visible light oxidation of polymers—Application to the photodegradation of MDMO-PPV10.1016/j.polymer.2008.04.001 ↗
42. Photo- and thermal degradation of MDMO-PPV: PCBM blends10.1016/j.solmat.2006.10.015 ↗
43. Reactive intermediates in the initiation step of the photo-oxidation of MDMO-PPV
44. Photo- and thermo-oxidation of poly(p-phenylene-vinylene) and phenylene-vinylene oligomer10.1016/j.polymdegradstab.2011.02.002 ↗
45. Imaging local trap formation in conjugated polymer solar cells: a comparison of time-resolved electrostatic force microscopy and scanning Kelvin probe imaging10.1021/jp1056607 ↗